Hợp kim cứng2023

Đo cỡ hạt WC phương pháp cắt

HMM-200 đo cỡ hạt WC 0,4 μm theo GB/T 3488, lặp lại ±0,03 μm.

Công ty
Nhà máy hợp kim cứng, Trung Trung Quốc
Địa chỉ
Hồ Nam
Danh mục
Kính hiển vi
Đo cỡ hạt WC phương pháp cắt
±0.03 μmĐộ lặp lại

Developing a 0.4 μm ultrafine grade, the plant outsourced grain sizing to SEM labs with a one-week turnaround, too slow for lot release.

Solution: the HMM-200 microscope with a 100X/1.25 high-NA objective applies the GB/T 3488 intercept method at 1500X, 3 fields per sample and no fewer than 100 intercepts per field, with automatic image analysis.

Result: measured grain size was 0.38-0.42 μm, within 5% of SEM, with ±0.03 μm repeatability. Lot release went from 7 days to same-day, saving about RMB 400,000 in annual testing fees.