Полупроводники2024

ICPS-7510 для ppt-металлов в сверхчистой воде

ICPS-7510 контролирует 26 металлов в сверхчистой воде на уровне нг/л; реакция на отклонения с 48 ч до 4 ч, брак по загрязнению нулевой.

Компания
Полупроводниковая фабрика, Вост. Китай
Адрес
Шанхай
ICPS-7510 для ppt-металлов в сверхчистой воде
0.5~2 ng/LТипичный предел обнаружения
4 hВремя реакции

The fab requires each metal below 10 ng/L in UPW and wet chemicals. Weekly outsourced ICP-MS checks lagged 48 hours, and a Cu excursion once scrapped an entire wafer lot.

Solution: an ICPS-7510 ICP-OES with micro-flow nebulization and auto-dilution monitors 26 elements (Fe, Cu, Na, Ca, Al) across six media including UPW, ammonia and hydrogen peroxide, at typical 0.5-2 ng/L detection limits, three runs daily.

Results: deviation versus outsourced ICP-MS stayed under 10%, and response time fell from 48 to 4 hours. In the first six months it caught three slow Na and Si rises from failing resin columns; contamination-driven lot scrap went to zero, avoiding over ten million yuan of annual loss.