ICPS-7510 monitors 26 metals such as Fe, Cu and Na in UPW and wet chemicals at ng/L detection limits, replacing outsourced ICP-MS; response fell from 48 h to 4 h and contamination scrap went to zero.

Company
A wafer fab, E. China
Address
Shanghai
ICPS-7510 for ppt-Level Metals in Semiconductor UPW
0.5~2 ng/LTypical detection limit
4 hResponse time

The fab requires each metal below 10 ng/L in UPW and wet chemicals. Weekly outsourced ICP-MS checks lagged 48 hours, and a Cu excursion once scrapped an entire wafer lot.

Solution: an ICPS-7510 ICP-OES with micro-flow nebulization and auto-dilution monitors 26 elements (Fe, Cu, Na, Ca, Al) across six media including UPW, ammonia and hydrogen peroxide, at typical 0.5-2 ng/L detection limits, three runs daily.

Results: deviation versus outsourced ICP-MS stayed under 10%, and response time fell from 48 to 4 hours. In the first six months it caught three slow Na and Si rises from failing resin columns; contamination-driven lot scrap went to zero, avoiding over ten million yuan of annual loss.