Surface hardness of nitrided thin-wall cylinders with superficial Rockwell
80 → 18 μmIndent depth
≤1.5 HRCVs. HV1
40 → 22 sCycle

Cylinders have 3.5 mm walls and a 0.25 mm nitrided case. Standard Rockwell at 150 kg drove the indent 80 µm deep, a third of the case, denting the thin wall and reading low.

Solution: HRC-45M superficial Rockwell at 15N (147 N total), giving an 18 µm indent well inside the case; HV1 on HBRVS-187.5 was used as a cross-check to build a plant conversion table.

Result: 18 µm indents with no distortion, conversion within 1.5 HRC of HV1 versus 4 HRC previously, cycle time down from 40 to 22 seconds, and no more extra bosses left just for hardness testing.