Автомобилестроение2025

100% сортировка пружин подвески по нагрузке

YRWT-M100: нагрузка и жёсткость за 12 с, погрешность ±0,5%, 3 группы.

Компания
Завод рессор подвески, Вост. Китай
Адрес
Ханчжоу, Чжэцзян
100% сортировка пружин подвески по нагрузке
60 → 12 sВремя на пружину
0.9% → 0.05%Брак по высоте

MacPherson-strut coil springs must hold load within ±4% at a specified height. With only 5% sampling, left-right ride-height complaints clustered after vehicle assembly; 100% sorting was needed but the old tester took a minute per spring.

Solution: a YRWT-M100 computer-controlled spring tension/compression tester, 100 kN class 0.5, with self-levelling compression plates. The program sets two test heights, computes load and stiffness automatically, sorts into grades A/B/C by deviation and triggers marking.

Result: 12 seconds per spring with load indication error within ±0.5% (verified to JJG 139); after 100% sorting, the out-of-tolerance rate for left-right height difference fell from 0.9% to 0.05%.

Benefit: full inspection replaced sampling with no extra labour, and suspension-related warranty complaints dropped 70% quarter on quarter.

⇄0СравнениеСравнение характеристик