Ô tô2025

Phân loại toàn phần tải lò xo treo

YRWT-M100 đo tải và độ cứng trong 12 giây, chia 3 nhóm.

Công ty
Nhà máy lò xo treo ô tô, Đông Trung Quốc
Địa chỉ
Hàng Châu, Chiết Giang
Phân loại toàn phần tải lò xo treo
60 → 12 sThời gian/lò xo
0.9% → 0.05%Tỷ lệ lỗi chênh cao

MacPherson-strut coil springs must hold load within ±4% at a specified height. With only 5% sampling, left-right ride-height complaints clustered after vehicle assembly; 100% sorting was needed but the old tester took a minute per spring.

Solution: a YRWT-M100 computer-controlled spring tension/compression tester, 100 kN class 0.5, with self-levelling compression plates. The program sets two test heights, computes load and stiffness automatically, sorts into grades A/B/C by deviation and triggers marking.

Result: 12 seconds per spring with load indication error within ±0.5% (verified to JJG 139); after 100% sorting, the out-of-tolerance rate for left-right height difference fell from 0.9% to 0.05%.

Benefit: full inspection replaced sampling with no extra labour, and suspension-related warranty complaints dropped 70% quarter on quarter.

⇄0So sánhSo sánh thông số