Металлургия стали2024

Спектрометр Q8 для экспресс-анализа стали за 40 с

Спектрометр Q8 анализирует 22 элемента за 40 с, предел обнаружения C 0,001%; пересорт снижен с 1,8% до 0,4%.

Компания
Завод толстолистовой стали, Сев. Китай
Адрес
Таншань, Хэбэй
Спектрометр Q8 для экспресс-анализа стали за 40 с
40 sВремя анализа
0.4%Пересорт

Melting high-strength grades such as Q690, the mill sent ladle samples to a central XRF lab - a 12-minute round trip that forced the tap schedule to wait, and off-spec chemistry caused a 1.8% regrading rate.

Solution: a floor-standing Q8 OES installed in the melt-shop lab, spark-excited under argon, reporting 22 elements (C, Si, Mn, P, S, Cr, Ni, Mo and more) in 40 seconds with a 0.001% carbon detection limit; a built-in grade library judges conformance and carbon equivalent on the spot.

Results: measure-and-judge at the furnace cut regrading from 1.8% to 0.4% and saved 8 minutes per heat - about 21000 extra tonnes of conforming product a year at 1.2 Mt capacity. Correlation with XRF held within 0.005% C and 0.02% Mn, passing CNAS audit.