Steel and metallurgy2024

Q8 OES for 40 s Ladle Analysis of Special Steel

Q8 OES completes 22-element ladle analysis in 40 s with 0.001% carbon detection limit; regrading fell from 1.8% to 0.4% and each heat saves 8 minutes of waiting.

会社名
A special-steel plate mill, N. China
所在地
Tangshan, Hebei
Q8 OES for 40 s Ladle Analysis of Special Steel
40 sAnalysis time
0.4%Regrading rate

Melting high-strength grades such as Q690, the mill sent ladle samples to a central XRF lab - a 12-minute round trip that forced the tap schedule to wait, and off-spec chemistry caused a 1.8% regrading rate.

Solution: a floor-standing Q8 OES installed in the melt-shop lab, spark-excited under argon, reporting 22 elements (C, Si, Mn, P, S, Cr, Ni, Mo and more) in 40 seconds with a 0.001% carbon detection limit; a built-in grade library judges conformance and carbon equivalent on the spot.

Results: measure-and-judge at the furnace cut regrading from 1.8% to 0.4% and saved 8 minutes per heat - about 21000 extra tonnes of conforming product a year at 1.2 Mt capacity. Correlation with XRF held within 0.005% C and 0.02% Mn, passing CNAS audit.

⇄0比較仕様比較