MARSURF-LD260 для волнистости торцов уплотнений

MARSURF-LD260 заменил интерференционные полосы измерением 0,1 мкм; волнистость 0,4 мкм, утечки снижены на 80%.

Компания
Институт уплотнительной техники, Вост. Китай
Адрес
Ханчжоу, Чжэцзян
MARSURF-LD260 для волнистости торцов уплотнений
0.4 μmВолнистость торца
0.5%Ранние утечки

Seal faces were judged by monochromatic interference bands, one band equalling 0.3 um. Reading bands was empirical - two inspectors could differ by a whole band - and waviness and convergence taper could not be quantified. Early pump seal leakage ran at 2.5%.

Solution: a MARSURF-LD260 profile measurement system traces radially across the face with 0.1 um straightness uncertainty. Software separates the waviness component (2-15 UPR) from taper, outputting quantitative waviness amplitude and convergence angle.

Results: with face waviness tightened to 0.4 um and convergence taper held at 0.6-1.2 um per 10 mm, the lapping process is now corrected closed-loop from data. Early leakage fell from 2.5% to 0.5% and operator-to-operator reading differences disappeared entirely.