Automotive gears2025

Hardness sampling and data upload on a gear-shaft heat-treat line

HRC-150SMJ with direct MES upload measures 18 seconds per part, storing data automatically so an out-of-spec reading traces back to a furnace batch within five minutes.

Компания
Gearbox gear plant, Chongqing
Адрес
Chongqing
Категория
Твердомеры
Hardness sampling and data upload on a gear-shaft heat-treat line
35 → 18 sPer part
次日 → 5 minTrace time
约 600 件Rework avoided

Gear shafts require 58–62 HRC at the surface and 30–42 HRC at the core after carburising and quenching. Manual Rockwell readings went onto paper and were typed into Excel the next day, so by the time an anomaly appeared hundreds of parts had been made.

Solution: HRC-150SMJ digital motorised Rockwell with a V-block support; the operator loads the part and presses start for an automatic load-dwell-unload-read cycle in 18 seconds, with hardness, time, operator and part QR code written to MES over Ethernet.

Result: 18 seconds per part instead of 35, with all 40 samples per shift stored automatically; one 56.5 HRC reading triggered an immediate alarm and traced to quenching-oil temperature on furnace 3 within five minutes, avoiding about 600 reworked parts.

⇄0СравнениеСравнение характеристик