Foundry2024

Brinell hardness and gradients in ductile-iron castings

HBRVS-187.5 with HBW 2.5/187.5 measures six points per casting in eight minutes, converting to tensile strength within 12 MPa.

Компания
Wind-power castings plant, Shandong
Адрес
Weifang, Shandong
Категория
Твердомеры
Brinell hardness and gradients in ductile-iron castings
8 min(6 点)Per casting
22 → 11HBW spread
≤12 MPaStrength conversion

Wind-turbine hubs require 180–240 HBW in the body with wall thickness varying from 30 to 120 mm, so cooling rate differs by location. Testing a single point on a attached block did not represent the body, and customers demanded body measurements.

Solution: HBRVS-187.5 in Brinell mode at HBW 2.5/187.5 with a portable grinding station; six points per casting (flange, hub wall, fillet, two each), recorded and plotted as a gradient map.

Result: eight minutes per casting; the initial 22 HBW spread pointed to slow cooling in thick sections and fell to 11 HBW after chills were repositioned; conversion to tensile strength is within 12 MPa, fast enough to decide whether destructive sampling is needed.

⇄0СравнениеСравнение характеристик