GCr15 bearing rings are inclusion-rated per GB/T 10561 method A. Hand preparation dragged oxides and silicates into comet tails or pulled them out as pits, swinging DS ratings between 0.5 and 1.0 - customers disputed results on the same material lot.

Solution: an HXZMP-2000Z automatic grinder-polisher with single-point pressure and counter-rotation runs a short diamond sequence of 9, 3 and 1 um, finishing with a 40-second 0.05 um alumina polish so inclusions stay in place.

Results: six-field ratings at 100X hold stable at DS class 1.0 with 100% agreement against third-party referee samples. Disputed batches fell from two or three per quarter to zero, prep labour dropped from two operators to half, saving about 250000 yuan of re-testing a year.