Bearing manufacturing2023

HXZMP-2000Z Prep Keeps Bearing Steel Inclusions Intact

HXZMP-2000Z automatic preparation of GCr15 bearing rings avoids inclusion pull-out and drag; DS class 1.0 ratings per GB/T 10561 are stable with 100% agreement against referee samples, ending quarterly inclusion complaints.

会社名
A precision bearing plant, E. China
所在地
Ningbo, Zhejiang
HXZMP-2000Z Prep Keeps Bearing Steel Inclusions Intact
1.0 级DS inclusion class
100%Referee agreement

GCr15 bearing rings are inclusion-rated per GB/T 10561 method A. Hand preparation dragged oxides and silicates into comet tails or pulled them out as pits, swinging DS ratings between 0.5 and 1.0 - customers disputed results on the same material lot.

Solution: an HXZMP-2000Z automatic grinder-polisher with single-point pressure and counter-rotation runs a short diamond sequence of 9, 3 and 1 um, finishing with a 40-second 0.05 um alumina polish so inclusions stay in place.

Results: six-field ratings at 100X hold stable at DS class 1.0 with 100% agreement against third-party referee samples. Disputed batches fell from two or three per quarter to zero, prep labour dropped from two operators to half, saving about 250000 yuan of re-testing a year.

⇄0比較仕様比較