기술 자료415 views

Surface Lay Direction and Fit Performance: Why Tool-Mark Orientation Affects Sealing

At the same Ra, lay parallel to sliding breaks in faster while cross-lay leaks more; lay direction matters as much as Ra.

华旋光电技术部
Surface Lay Direction and Fit Performance: Why Tool-Mark Orientation Affects Sealing

Lay symbols

GB/T 131 defines lay symbols: = parallel to the projection direction, ⊥ perpendicular, × crossed, M multidirectional, C circular, R radial, P particulate. Turned cylinders carry circumferential lay, surface grinding gives a single parallel lay, lapping a multidirectional one. The lay symbol beside the Ra value on a drawing is often overlooked, yet it is a design requirement equal to the number.

Effect on sealing

Sealing faces fear through-channels: scratches and lay running radially across the sealing line form leak paths, and a face can leak despite meeting Ra. Static flanges want circular lay (C); the spiral from continuous turning feed is exactly the hazard, so finishing should break spiral continuity. Dynamic sealing journals at lip seals must be spiral-free — spiral lay pumps oil like a screw thread, leaking in one rotation direction; shafts rotating both ways need plunge grinding.

Effect on friction and fits

On sliding bearings and guideways, lay parallel to sliding breaks in faster, lowers friction and builds the oil film readily; cross-lay raises initial wear by more than 30 percent in classic experiments. On interference fits, circumferential lay scrapes particles during pressing, cutting effective interference by 5-10 percent and scattering press force. Honing cross-hatch (symbol ×, 30-60 degree angles) is the classic oil-retaining texture for cylinder bores, and its plateau-honed bearing-ratio curve, the Rk family, describes function far better than Ra alone.

Measurement notes

A stylus instrument must traverse perpendicular to the lay by default; tracing along the lay misses valley depth and under-reports Ra by 20-50 percent. On multidirectional lapped surfaces, measure two perpendicular directions and take the larger value. For sealing faces, add RSm, mean spacing of profile elements, and bearing-ratio parameters, because Ra alone cannot characterize texture.