Pressure vessels & welding2024

Macro/micro section line for welding PQR

An HXZDQ-160 + HXQ-100 + HXZMP-2000 line raised PQR section acceptance from 85% to 99%.

회사명
Pressure vessel fabricator, Shandong
주소
Jinan, Shandong
Macro/micro section line for welding PQR
99%First-pass acceptance
6 dCycle time saved

Hand-cut and ground PQR sections were frequently rejected for burn marks and residual scratches, delaying qualification.

Solution: HXZDQ-160 water-cooled cutting with controlled feed, HXQ-100 hydraulic mounting for parallel weld sections, and an HXZMP-2000 "low-carbon PQR" program: 320→1200 grit then 3/1 µm diamond, etched 6 s in 4% nital.

Result: 99% first-pass acceptance, clear lack-of-fusion evidence on macro sections and clean two-phase micrographs — six working days saved per qualification.