Construction machinery2023

Tensile verification of track chains and pins for construction machinery

WEW600-1000D computerised hydraulic machine tests full track-chain tension and pin shear, 600 kN class 1, replacing a lever-type legacy machine, with data accepted by the OEM.

회사명
A construction-machinery supplier, E. China
주소
Xuzhou, Jiangsu
카테고리
Testing Machines
Tensile verification of track chains and pins for construction machinery
486 kNChain breaking force
6 kNLot range

Excavator track chains break above 400 kN in full-chain tension. The legacy lever-type machine read from a dial with no loading-rate control, so breaking data scattered widely and the OEM refused to accept them.

Solution: a WEW600-1000D computerised hydraulic universal testing machine, 600 kN class 1, with flat-pull chain fixtures and pin-shear accessories. Loading runs at a constant 10 kN/s per the company standard, with force-displacement curves recorded and archived.

Result: the full chain broke at 486 kN, 15% above the design value; pin single-shear measured 312 kN with a 6 kN spread across five pieces from the same lot, a clear improvement in consistency.

Benefit: the OEM accepted the data and listed the plant as an approved supplier, adding about CNY 8 million in annual orders.