WAW-1000D Electro-hydraulic Servo Universal Testing Machine

Electro-hydraulic Servo Universal Testing Machine

型番WAW-1000D
  • 试验力测量范围50~1000kN
  • 试验力示值相对误差≤示值的±1%
  • 试验力分辨率0.01kN
  • 位移测量分辨力0.01mm

By submitting you agree to our privacy policy.

01

製品概要

◆该试验机采用微机控制全数字宽频电液数字阀,驱动精密液压缸,对试验力、位移、变形进行多种模式的自动控制,完成对试样的拉伸、压缩、抗弯试验,符合国家标准GB/T228.1-2010《金属材料室温拉伸试验方法》的要求及其他标准要求。
◆试验机主机采用液压缸下置式;调整试验空间的动力及传动装置安装在试验机底部,传动平稳;上下钳口座为全开式结构,自动液压加紧系统,装夹试样方便,稳定性好。
◆.采用联想品牌微机,完成试验过程中试验参数的设定、试验过程的控制、数据采集、处理、分析、存储及显示(试验数据包括:材料抗拉强度、弹性模量、延伸率、屈服强度、规定塑性延伸强度等)、控制及测量精密、准确。
技术参数:
最大试验力
1000kN
试验力测量范围
50~1000kN
试验力示值相对误差
≤示值的±1%
试验力分辨率
0.01kN
位移测量分辨力
0.01mm
变形测量精度
0.01mm
最大拉伸试验空间
750mm
最大压缩空间
380mm
活塞行程
150mm
圆试样钳口夹持直径
Φ13-Φ40mm
扁试样钳口夹持厚度
0-15mm
扁试样最大夹持宽度
75mm
压盘尺寸
φ160mm
弯曲试验两点间最大距离
450mm
弯曲支滚宽度
140mm
弯曲支滚直径
Φ40mm
活塞最大移动速度
50mm/min
夹紧方式
自动加紧
主机外形尺寸
900×710×2200mm
测力柜外形尺寸
1000×700×1400mm
重量
4000kg

WAW-1000D Electro-hydraulic Servo Universal Testing Machine supplied by CHWES. 20 key specifications available on request.

02

仕様

试验力测量范围50~1000kN
试验力示值相对误差≤示值的±1%
试验力分辨率0.01kN
位移测量分辨力0.01mm
变形测量精度0.01mm
最大拉伸试验空间750mm
最大压缩空间380mm
活塞行程150mm
圆试样钳口夹持直径Φ13-Φ40mm
扁试样钳口夹持厚度0-15mm
扁试样最大夹持宽度75mm
压盘尺寸φ160mm
弯曲试验两点间最大距离450mm
弯曲支滚宽度140mm
弯曲支滚直径Φ40mm
活塞最大移动速度50mm/min
夹紧方式自动加紧
主机外形尺寸900×710×2200mm
测力柜外形尺寸1000×700×1400mm
重量4000kg

* Generated by rule engine over the product database; for pre-selection only.

03

測定原理

A universal testing machine comprises the load frame, drive system, load cell, displacement/extensometer measurement and closed-loop control. A servo motor and screw drive the crosshead (or a servo valve drives the actuator); the load cell converts force to a signal, the extensometer measures strain over the gauge length, and the controller follows the programmed rate while logging force–displacement–strain.

Software derives upper and lower yield strength (ReH/ReL), tensile strength Rm, elongation A, reduction of area Z and modulus E. Control modes include speed, force, displacement and strain; GB/T 228.1-2021 requires strain control in the yield region (method A) for lower uncertainty.

  • Electromechanical: 1–600 kN for metals, plastics and composites.
  • Servo-hydraulic: 300–2000 kN for high-strength steel, fasteners and bars.
  • Specialised: friction and wear, impact, bend, peel.
04

Process animation

  1. Measure width and thickness (or diameter) at three points; compute S₀.
  2. Clamp with wedge or hydraulic grips, aligned to avoid bending.
  3. Extensometer attached to the gauge length, zeroed.
  4. Load: speed control in the elastic range, strain control at yield, speed control in hardening.
  5. Fracture: detect peak and break, stop.
  6. Report: ReH/ReL/Rm/A/Z with curves and data tables.
0102030405
05

Calculation & formulas

1. Tensile strength: Rm = Fmax/S0; a 10 mm bar (S0=78.5 mm²) breaking at 62.8 kN gives Rm ≈ 800 MPa.

2. Yield: Rp0.2 is interpolated from the extensometer curve at 0.2% non-proportional extension.

3. Elongation & reduction: A = (Lu−L0)/L0; Z = (S0−Su)/S0; L0=50, Lu=62.5 mm → A = 25%.

4. Friction coefficient: μ = F/N; at N = 100 N and F = 32 N, μ = 0.32. Four-ball results report PB (last non-seizure) and PD (weld) loads.

5. Wear rate: k = V/(F·s); obtain V from Δm/ρ. Typical specific wear rates run 10⁻⁸–10⁻⁶ mm³/(N·m).

06

規格

StandardTitleScope
GB/T 228.1-2021Metallic materials — tensile testing, room temperatureTension
ISO 6892-1Tensile testing at room temperatureExport projects
ASTM E8/E8MTension testing of metallic materialsAmericas
GB/T 7314-2017Compression testing at room temperatureCompression
GB/T 232-2010Bend testing of metallic materialsBending
GB/T 3098.1-2010Mechanical properties of fastenersFasteners
07

選定ガイド

1. Frame capacity plus 20–30%: Φ32 rebar yields near 630 kN so choose 1000 kN; M30 proof load is about 550 kN so choose 600–1000 kN. Running at full scale accelerates load-cell fatigue.

2. Servo-hydraulic or electromechanical: ≥300 kN with high stiffness and long stroke (rebar, bolts, concrete) needs servo-hydraulic (WAW/WEW); ≤300 kN with tight speed control (plastics, composites) suits electromechanical frames (WDS).

3. Display, digital or PC-controlled: a digital readout for single values; PC control (the -C suffix) for stress-strain curves, reports and batch data.

4. Fixtures often matter more than the frame: ribbed grips for rebar, proof-load fixtures for bolts, wrap grips for cables. Poor alignment costs 2–3 percentage points of elongation.

5. Extensometers and options: contact or video extensometers for modulus, high-temperature furnaces and extensometers, large platens with displacement control for battery crush.

6. Foundation and safety: a 1000 kN frame needs an isolated concrete base, guard doors and e-stops; hydraulic units need oil-temperature management.

SeriesTypeForce rangeTypical specimens
WDS-1G to 300GElectromechanical1–300 kNPlastics, composites, small parts
WEW-100D to 1000DHydraulic, digital100–1000 kNRebar, bolts, metals
WEW-300C to 2000CHydraulic, PC300–2000 kNHigh-strength bolts, forgings
WAW-100 to 1000Servo-hydraulic100–1000 kNRate-controlled acceptance
WAW-300C to 2000CServo-hydraulic, PC300–2000 kNBridges, nuclear components
WES-300C to 2000CCompression300–2000 kNConcrete, blocks
MMW-1A / MRS-10WFriction and wear—Lubricants, coatings

Three acceptance checks: verify force at 20/50/80% with a standard load cell; check alignment so a standard specimen breaks mid-gauge; run three identical specimens and look at scatter.

08

試験方法

Specimen. Proportional (L₀ = 5.65√S₀) or non-proportional specimens to GB/T 228.1; transition radius R ≥ 5 mm; Ra ≤ 1.6 µm with work-hardened layers removed.

Measurement. Width and thickness at three positions within the gauge length, use the minimum for S₀; below 1 mm use optical or 0.001 mm micrometers.

Loading. 5–30 MPa/s in the elastic range, 0.00025/s strain rate at yield per method A, up to 0.0067/s in hardening; log at 100 Hz or more to catch yield serrations.

Evaluation. ReH is the first peak, ReL the lowest point, Rm the maximum force over S₀, A from the final gauge length (offset method), Z from the minimum fracture diameter.

Quality control. Daily check with a reference specimen, monthly force calibration with a class 0.3 proving instrument, half-yearly extensometer calibration, 23 ± 5 °C.

09

Industry applications

  • Construction and bridges: rebar tensile and bend, high-strength bolt wedge load, strand relaxation, concrete compression, with loading-rate control to GB/T 228.1 and GB/T 3098.1.
  • Metals and forgings: room and elevated temperature tensile, yield strength, elongation and reduction of area for material verification.
  • Automotive parts: chassis tension-compression, suspension springs, seat-belt anchorages, battery-pack crush with dedicated fixtures.
  • Fasteners: proof load, nut proof load, washer elasticity; fixture alignment drives scatter.
  • Plastics and composites: tension, flexure, compression and shear on low-force frames (WDS) with non-contact extensometers.
  • Cables and ropes: breaking force and elongation with long stroke and large-deformation grips.
  • Friction and wear: MMW/MRS four-ball, reciprocating and ring-block tests for lubricants and coatings.
  • Third-party testing: calibrated frames with tamper-evident data and raw curve export.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0比較仕様比較