Construction steel2024

Combined tensile and bend testing of HRB400 rebar

WEW-1000D with ribbed grips and a bend attachment cuts a tensile-plus-bend set from 22 to 9 minutes, raising daily throughput 1.4 times.

会社名
Rebar processing centre, Sichuan
所在地
Chengdu, Sichuan
カテゴリ
Testing Machines
Combined tensile and bend testing of HRB400 rebar
22 → 9 minPer set
45 → 75Sets per day
8% → 0.5%Grip slip

The centre issues 60–80 rebar verification reports daily, each with two tensile and two bend specimens. Grips slipped, bars above Φ25 needed two people to align, and bending used a separate old machine, so one set took 22 minutes.

Solution: WEW-1000D with ribbed grips matched to the bar profile and a bend attachment using 3d/4d mandrels per GB/T 1499.2; the software computes yield, tensile strength and elongation and identifies the grade.

Result: nine minutes per set, daily throughput from 45 to 75 sets, grip slip from 8% to 0.5%, one operator can complete the set without changing machines, saving one headcount.

⇄0比較仕様比較