HXZDQ-160 Smart automatic metallographic cut-off machine

Complete metallographic specimen preparation

型番HXZDQ-160
  • Max specimen最大切割能力 φ160 mm
  • Control智能自动 / 全自动切割,闭环控制
  • Cooling循环冷却系统,防止试样过烧
  • Software制样工艺参数存储与调用

By submitting you agree to our privacy policy.

01

製品概要

The HXZDQ-160 provides programmable, repeatable metallographic specimen preparation.

The HXZDQ-160 provides programmable, repeatable metallographic specimen preparation.

02

仕様

Max specimen最大切割能力 φ160 mm
Control智能自动 / 全自动切割,闭环控制
Cooling循环冷却系统,防止试样过烧
Software制样工艺参数存储与调用

* Generated by rule engine over the product database; for pre-selection only.

03

測定原理

The goal of metallographic preparation is a flat, scratch-free mirror with intact edges and unchanged microstructure. The sequence is sectioning → mounting → grinding → polishing → etching, and every step affects the result.

Sectioning: diamond or alumina wheels with constant feed and abundant coolant to avoid heat-affected zones and deformation. Soft materials use resin-bonded wheels, hard materials metal-bonded diamond.

Mounting: hot mounting (phenolic, 130–180 °C, 20–30 MPa) is fast; cold mounting (epoxy/acrylic) suits temperature-sensitive materials and edge retention; copper-filled mounts allow electrolytic polishing.

Grinding and polishing: remove scratches step by step, each step fully erasing the previous one; diamond suspension 3 µm then 1 µm, final oxide polish. Soft materials need low pressure and short times to avoid relief.

04

Process animation

  1. Section: perpendicular cut, 0.5–2 mm/min feed with coolant.
  2. Mount: hot press at 150 °C/25 MPa for 8 min, or cold cure for 4 h.
  3. Rough grind: 320-grit SiC with water, remove cut marks.
  4. Fine grind: 600→800→1200 grit, 1–2 min each.
  5. Polish: 3 µm diamond, 1 µm diamond, oxide finish on a soft cloth at low pressure.
  6. Etch and inspect: 4% nital 3–8 s, dry, verify under the microscope.
0102030405
05

Calculation & formulas

1. Grinding allowance: each grade must remove 3–4× the previous scratch depth — 20–30 µm per grade (320→1200) for carbon steel; rotate the sample 90° at each change.

2. Burn-free cutting: keep feed low enough that chips do not blue (~300 °C); burned layers shift surface hardness by 2–5 HRC and show as tempered zones.

3. Hot mounting: phenolic at 150–165 °C, 250–300 bar, 5–8 min; use cold epoxy (24 °C/24 h or accelerated 60 °C/1 h) for quenched or aluminium parts.

4. Polishing time: removal ∝ P·n; typical 2–3 min at 3 µm diamond and 1–2 min at 1 µm — excess pressure causes smearing and pitting.

5. Etching quota: 4% nital 3–8 s for carbon steel; fix time, temperature and concentration per batch for comparability.

06

規格

StandardTitleUse
ASTM E3-11Guide for metallographic specimen preparationPreparation workflow
GB/T 13298-2015Examination of microstructureGeneral inspection
GB/T 15749-2008Quantitative metallographyQuantitative analysis
GB/T 10561-2005Non-metallic inclusion content in steelInclusions
ISO 4967Determination of non-metallic inclusionsExport projects
07

選定ガイド

1. Four linked steps: sectioning without deformation, mounting without voids and with edge protection, polishing without scratches or rounding, then etching and observation. A wrong choice at any step cannot be rescued by a better microscope.

2. Cutter by section size and heat sensitivity: abrasive cutters (HXQ-50/HXQ-100) for routine parts; low-speed precision sectioning with diamond or CBN wheels below 300 rpm for coatings, sheet and non-ferrous.

3. Mounting by batch and edge requirements: hot mounting (HXZDQ) is fast and cheap for routine parts; cold vacuum impregnation suits porous, coated and electronic samples.

4. Polishing by throughput: manual (HXZMP-1000) below 20 samples a day, semi-automatic (HXZMP-2000) for 20–80, automatic heads (HXZMP-3000) above 80 or where consistency matters.

5. Consumables matter more than the machine: grit sequence 180→400→800→1200→2000, diamond suspension 9→3→1 µm and the right cloth type must match, or you either cannot polish out or polish past the feature.

6. Room and safety: extraction and water for cutting and polishing, separate preparation and microscopy rooms, guards and e-stops on cutters.

EquipmentModelCapabilityUse
Precision cutterHXQ-50 / HXQ-100Low speed, no deformationCoatings, sheet, non-ferrous
Abrasive cutterHXGXSFast large-section cuttingRoutine steel parts
Hot mounting pressHXZDQ-100 / 110 / 120 / 160Φ25–Φ50 mountsBatch routine samples
Vacuum mountingHXZDQ-100ZVacuum impregnationPorous, coated, electronics
Manual polisherHXZMP-1000Single platenLow volume, teaching
Semi-automaticHXZMP-2000 / 2000ZTwin platen, timedMedium batches
AutomaticHXZMP-3000Multi-station, programmable forceHigh throughput, consistency
Electrolytic polish/etchHXSQ-100G / 100FDeformation-free surfaceStainless, nickel alloys

Why samples get scrapped: cutting heat alters the structure, mounting gaps cause edge smearing, over-polishing removes inclusions, over-etching blurs grain boundaries.

08

試験方法

Sampling. Choose a representative section (gear root, weld cross-section), cut perpendicular to the viewing plane, and record position and orientation.

Cutting. 0.5–2 mm/min feed, 2000–3000 rpm, abundant coolant; re-section if burn marks appear.

Mounting. Hot mount at 150 °C, 25 MPa for 8 min; cold epoxy cure 4 h (or 60 °C acceleration). Add a protective plate for coating cross-sections to prevent rounding.

Grinding and polishing. 320→600→800→1200, rinse and rotate 90° between steps; diamond 3 µm (3 min), 1 µm (2 min), oxide (1 min), decreasing force.

Check. Inspect unetched at 100× for scratches and edge rounding, then etch. Verify preparation quality daily with a reference sample.

09

Industry applications

  • Steel and automotive parts: batch preparation of carburised cases, weld joints and fasteners with no cutting deformation, void-free mounting and scratch-free polishing.
  • Non-ferrous and light alloys: aluminium and magnesium are prone to mechanical twinning and smearing, needing low-speed sectioning and dedicated polish.
  • Coatings and plating: thermal spray, PVD and electroplated cross-sections with edge protection (mounting plus nickel plating) to prevent rounding.
  • Electronics: PCB micro-sections, solder joints and BGA packages requiring precision cutting and vacuum resin mounting.
  • Additive manufacturing: porosity and melt-pool observation with traceable sampling position and direction.
  • Failure analysis: on-site sampling when the part cannot be shipped, fracture-surface protection and foreign-matter extraction.
  • Research and teaching: parallel samples, recorded parameters and reproducible results.
  • Third-party labs: 50–200 samples per day with stable cycle time and controlled consumable cost.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0比較仕様比較