The centre issues 60–80 rebar verification reports daily, each with two tensile and two bend specimens. Grips slipped, bars above Φ25 needed two people to align, and bending used a separate old machine, so one set took 22 minutes.
Solution: WEW-1000D with ribbed grips matched to the bar profile and a bend attachment using 3d/4d mandrels per GB/T 1499.2; the software computes yield, tensile strength and elongation and identifies the grade.
Result: nine minutes per set, daily throughput from 45 to 75 sets, grip slip from 8% to 0.5%, one operator can complete the set without changing machines, saving one headcount.