Machine tools2023

XZ-400 Profilometer for Gothic-Arc Raceway Profiles

XZ-400 scans gothic-arc raceways over 400 mm travel at 0.02 um resolution, replacing template light-gap checks; profile error converged from 4 um to 1.8 um, improving preload interchangeability.

会社名
A linear guideway maker, E. China
所在地
Nanjing, Jiangsu
XZ-400 Profilometer for Gothic-Arc Raceway Profiles
1.8 μmRaceway profile error
99.5%Interchangeable fit yield

Ground gothic-arc raceways were inspected with templates and light gaps, relying on inspectors to estimate 2-4 um clearances. Slider preload scattered and customers complained about poor interchangeability.

Solution: an XZ-400 long-travel profilometer covering all rail sizes over 400 mm, with 0.02 um Z resolution. A dedicated raceway fixture positions the rail, the stylus traces across the groove, and software fits the theoretical double arc, outputting profile error, arc radius deviation and groove span.

Results: raceway profile error converged from 4 um to 1.8 um and double-arc center distance was held within ±2 um. Slider preload scatter fell 55%, and first-pass yield of arbitrary rail-slider matching rose from 92% to 99.5%.

⇄0比較仕様比較