Automotive parts2025

Case depth and martensite rating for carburised gears

With the HX-G3A inverted microscope and analysis software, sample preparation plus case-depth measurement dropped from 45 to 18 minutes per gear, with repeatability within 0.02 mm.

会社名
Gearbox manufacturer, East China
所在地
Suzhou, Jiangsu
カテゴリ
Microscopes
Case depth and martensite rating for carburised gears
18 minTime per part
±0.02 mmRepeatability

The plant audits 30 carburised gears per day. With the previous upright microscope, specimens had to be sectioned from the tooth tip and re-mounted, and edge rounding inflated case depth by 0.03–0.05 mm; etching time was operator-dependent, so martensite ratings varied between batches.

Solution: an HX-G3A trinocular inverted microscope, specimens placed directly without re-mounting, 5×/10×/50× objectives, a 5 MP camera, and software modules for effective case depth to 550 HV1 (GB/T 9450) and martensite/retained austenite rating, with a fixed 5 s nital etch.

Result: 18 minutes per part, repeatability within 0.02 mm, 0.01 mm deviation versus a third-party laboratory, automatic monthly reports and audit traceability reduced from two days to two hours.

⇄0比較仕様比較