Connectors2023

HXQ-50 Hot Mounting for Connector Crimp Cross-Sections

HXQ-50 hot mounting at 180°C/25 MPa prepares connector crimp cross-sections; polished sections read 82% compression and 3% porosity, replacing hand-held grinding with a 12-minute cycle and two-week-early die wear warnings.

会社名
An automotive connector maker, S. China
所在地
Shenzhen, Guangdong
HXQ-50 Hot Mounting for Connector Crimp Cross-Sections
82%Wire compression
12 minSection cycle time

Crimp quality on automotive terminals was checked only by pull tests - internal voids and wire compression were invisible, so die wear was found only at failure, and over-resistance crimps once escaped in volume.

Solution: an HXQ-50 automatic hot mounter embeds Φ0.5 mm terminals at 180°C and 25 MPa for 5 minutes without collapsing the crimp. Sections polished to 1 um are read at 100X for wire compression ratio, porosity and wing engagement; three sections per shift.

Results: compression holds at 82% with 3% porosity, and trend data warns of crimp die wear two weeks early. Over-resistance escapes went to zero, section analysis runs at 12 minutes per piece, and about 900000 yuan of claims are avoided a year.

⇄0比較仕様比較