HXZMP-1000Z Prep for Forging Flow Lines and Coarse Rings

HXZMP-1000Z automatic prep with caustic etch reveals flow-line continuity and 0.8 mm coarse-grain rings on 7075 forgings; disputed acceptance batches fell from 8 a year to 1.

会社名
An aerospace forging plant, SW. China
所在地
Deyang, Sichuan
HXZMP-1000Z Prep for Forging Flow Lines and Coarse Rings
0.8 mmCoarse ring depth
18 minPrep time per part

7075 aerospace forgings are accepted per GJB on flow-line continuity and coarse-grain ring depth. Hand-ground macro samples kept scratches, and after caustic etch two inspectors could reach different verdicts - eight disputed batches a year needed third-party re-tests.

Solution: an HXZMP-1000Z automatic grinder-polisher with programmed pressure and speed, grinding to 1200 grit then a 3 um polish for a scratch-free surface; etching in 20% NaOH at 70°C for 90 s gives uniform contrast of flow lines and the coarse ring.

Results: the 0.8 mm coarse-grain ring is clearly measurable and cut-flow criteria are unified; disputed batches fell to one a year. Macro prep time per piece dropped from 50 to 18 minutes, saving about 400000 yuan of third-party re-testing annually.