HXGXS Metallographic image analysis software

Complete metallographic specimen preparation

ModelHXGXS
  • Software晶粒度/层深/夹杂物评级,GB/T 6394、GB/T 10561
  • Control适配 HX 系列金相显微镜与工业相机
  • Profile parameters报告导出、标定与数据库管理

By submitting you agree to our privacy policy.

01

Overview

The HXGXS provides programmable, repeatable metallographic specimen preparation.

The HXGXS provides programmable, repeatable metallographic specimen preparation.

02

Specifications

Software晶粒度/层深/夹杂物评级,GB/T 6394、GB/T 10561
Control适配 HX 系列金相显微镜与工业相机
Profile parameters报告导出、标定与数据库管理

* Generated by rule engine over the product database; for pre-selection only.

03

Working principle

The goal of metallographic preparation is a flat, scratch-free mirror with intact edges and unchanged microstructure. The sequence is sectioning → mounting → grinding → polishing → etching, and every step affects the result.

Sectioning: diamond or alumina wheels with constant feed and abundant coolant to avoid heat-affected zones and deformation. Soft materials use resin-bonded wheels, hard materials metal-bonded diamond.

Mounting: hot mounting (phenolic, 130–180 °C, 20–30 MPa) is fast; cold mounting (epoxy/acrylic) suits temperature-sensitive materials and edge retention; copper-filled mounts allow electrolytic polishing.

Grinding and polishing: remove scratches step by step, each step fully erasing the previous one; diamond suspension 3 µm then 1 µm, final oxide polish. Soft materials need low pressure and short times to avoid relief.

04

Process animation

  1. Section: perpendicular cut, 0.5–2 mm/min feed with coolant.
  2. Mount: hot press at 150 °C/25 MPa for 8 min, or cold cure for 4 h.
  3. Rough grind: 320-grit SiC with water, remove cut marks.
  4. Fine grind: 600→800→1200 grit, 1–2 min each.
  5. Polish: 3 µm diamond, 1 µm diamond, oxide finish on a soft cloth at low pressure.
  6. Etch and inspect: 4% nital 3–8 s, dry, verify under the microscope.
0102030405
05

Calculation & formulas

1. Grinding allowance: each grade must remove 3–4× the previous scratch depth — 20–30 µm per grade (320→1200) for carbon steel; rotate the sample 90° at each change.

2. Burn-free cutting: keep feed low enough that chips do not blue (~300 °C); burned layers shift surface hardness by 2–5 HRC and show as tempered zones.

3. Hot mounting: phenolic at 150–165 °C, 250–300 bar, 5–8 min; use cold epoxy (24 °C/24 h or accelerated 60 °C/1 h) for quenched or aluminium parts.

4. Polishing time: removal ∝ P·n; typical 2–3 min at 3 µm diamond and 1–2 min at 1 µm — excess pressure causes smearing and pitting.

5. Etching quota: 4% nital 3–8 s for carbon steel; fix time, temperature and concentration per batch for comparability.

06

Standards

StandardTitleUse
ASTM E3-11Guide for metallographic specimen preparationPreparation workflow
GB/T 13298-2015Examination of microstructureGeneral inspection
GB/T 15749-2008Quantitative metallographyQuantitative analysis
GB/T 10561-2005Non-metallic inclusion content in steelInclusions
ISO 4967Determination of non-metallic inclusionsExport projects
07

Selection guide

1. Four linked steps: sectioning without deformation, mounting without voids and with edge protection, polishing without scratches or rounding, then etching and observation. A wrong choice at any step cannot be rescued by a better microscope.

2. Cutter by section size and heat sensitivity: abrasive cutters (HXQ-50/HXQ-100) for routine parts; low-speed precision sectioning with diamond or CBN wheels below 300 rpm for coatings, sheet and non-ferrous.

3. Mounting by batch and edge requirements: hot mounting (HXZDQ) is fast and cheap for routine parts; cold vacuum impregnation suits porous, coated and electronic samples.

4. Polishing by throughput: manual (HXZMP-1000) below 20 samples a day, semi-automatic (HXZMP-2000) for 20–80, automatic heads (HXZMP-3000) above 80 or where consistency matters.

5. Consumables matter more than the machine: grit sequence 180→400→800→1200→2000, diamond suspension 9→3→1 µm and the right cloth type must match, or you either cannot polish out or polish past the feature.

6. Room and safety: extraction and water for cutting and polishing, separate preparation and microscopy rooms, guards and e-stops on cutters.

EquipmentModelCapabilityUse
Precision cutterHXQ-50 / HXQ-100Low speed, no deformationCoatings, sheet, non-ferrous
Abrasive cutterHXGXSFast large-section cuttingRoutine steel parts
Hot mounting pressHXZDQ-100 / 110 / 120 / 160Φ25–Φ50 mountsBatch routine samples
Vacuum mountingHXZDQ-100ZVacuum impregnationPorous, coated, electronics
Manual polisherHXZMP-1000Single platenLow volume, teaching
Semi-automaticHXZMP-2000 / 2000ZTwin platen, timedMedium batches
AutomaticHXZMP-3000Multi-station, programmable forceHigh throughput, consistency
Electrolytic polish/etchHXSQ-100G / 100FDeformation-free surfaceStainless, nickel alloys

Why samples get scrapped: cutting heat alters the structure, mounting gaps cause edge smearing, over-polishing removes inclusions, over-etching blurs grain boundaries.

08

Test method

Sampling. Choose a representative section (gear root, weld cross-section), cut perpendicular to the viewing plane, and record position and orientation.

Cutting. 0.5–2 mm/min feed, 2000–3000 rpm, abundant coolant; re-section if burn marks appear.

Mounting. Hot mount at 150 °C, 25 MPa for 8 min; cold epoxy cure 4 h (or 60 °C acceleration). Add a protective plate for coating cross-sections to prevent rounding.

Grinding and polishing. 320→600→800→1200, rinse and rotate 90° between steps; diamond 3 µm (3 min), 1 µm (2 min), oxide (1 min), decreasing force.

Check. Inspect unetched at 100× for scratches and edge rounding, then etch. Verify preparation quality daily with a reference sample.

09

Industry applications

  • Steel and automotive parts: batch preparation of carburised cases, weld joints and fasteners with no cutting deformation, void-free mounting and scratch-free polishing.
  • Non-ferrous and light alloys: aluminium and magnesium are prone to mechanical twinning and smearing, needing low-speed sectioning and dedicated polish.
  • Coatings and plating: thermal spray, PVD and electroplated cross-sections with edge protection (mounting plus nickel plating) to prevent rounding.
  • Electronics: PCB micro-sections, solder joints and BGA packages requiring precision cutting and vacuum resin mounting.
  • Additive manufacturing: porosity and melt-pool observation with traceable sampling position and direction.
  • Failure analysis: on-site sampling when the part cannot be shipped, fracture-surface protection and foreign-matter extraction.
  • Research and teaching: parallel samples, recorded parameters and reproducible results.
  • Third-party labs: 50–200 samples per day with stable cycle time and controlled consumable cost.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0CompareProduct comparison