HBE-3000C Brinell Hardness Tester

Brinell Hardness Tester

ModelHBE-3000C

    By submitting you agree to our privacy policy.

    01

    Overview

    HBE-3000C简易数显布氏硬度计采用5寸彩色触摸屏不用查表,键入压痕直径长度,触摸屏直接显示硬度值;主要用于铸铁、钢材、有色金属及软合金等材料的硬度测定,布氏硬度试验是所有硬度试验中压痕最大的一种试验法,它能反映出材料的综合性能,不受试样组织显微偏析及成分不均匀的影响,所以它是一种精度较高的硬度试验法。在冶金、锻造、未经淬火钢及有色金属等工业领域、实验室、大专院校和科研单位内广泛使用。
    产品特点:
    型号
    HBE‑3000C
    测量标尺
    HBW2.5/62.5、HBW2.5/187.5、HBW5/62.5、HBW5/125、HBW5/250、HBW5/750、HBW10/100、HBW10/250、HBW10/500、HBW10/1000、HBW10/1500、HBW10/3000
    试验力级数
    62.5kgf
    (612.5N)、100kgf(980N)、125kgf(1225N)、187.5kgf(1837.5N)、250kgf(2450N)、500kgf(4900N)、750kgf(7350N)、1000kgf(9800N)、1500kgf(14700N)、3000Kgf(29400N)
    转换标尺
    HRC、HV、HK、HBW、HRA、HRD、HR15N、HR30N、HR45N、HR15T、HR30T、HR45T、HRB、HRF
    加载机构
    电机加载
    试验力加载
    自动(加载/保荷/卸载)
    执行国家标准
    GB/T231.1 国家标准,GB/T231.2 国家标准,JJG150 检定规程
    读数方式
    毂轮读数
    视场的有效测量范围
    6mm
    理论硬度测量范围
    8‑650HBW
    硬度值显示方式
    触摸屏(4.3 寸)直接显示结果
    读数目镜放大倍率
    20X
    读数目镜最小分值
    0.01mm
    试验力保荷时间
    0‑60 秒,最小变动量 1 秒
    试件最大高度
    250mm
    压头中心到内壁距离
    155mm
    测试记录
    0‑30 组
    试台直径
    大平台 φ200mm、中平台 φ77mm、V 型台 φ77mm
    电源电压
    AC 220V/50Hz
    外形尺寸
    512*223*745mm(长 * 宽 * 高)
    净重
    114.0kg
    毛重
    139.5kg

    HBE-3000C Brinell Hardness Tester supplied by CHWES. 0 key specifications available on request.

    02

    Specifications

    * Generated by rule engine over the product database; for pre-selection only.

    03

    Working principle

    Hardness testing presses an indenter into the surface under a constant load and converts indentation size or depth into a hardness value. Vickers uses a 136° diamond pyramid: HV = 0.1891 × F(N)/d²(mm), where d is the mean diagonal.

    Hot hardness is performed in vacuum or high-purity inert gas. Specimen and indenter are heated independently and must be at the same temperature or corrected per the standard; loading, dwell and unloading all happen inside the hot zone, and the indentation is measured through a high-temperature optic or after cooling. The HMAS series uses a uniform hot zone with ±5 °C uniformity from 200 to 1600 °C.

    • Vickers 0.01–100 kgf: full range, thin layers and case-depth gradients.
    • Rockwell C 150 kgf: fast batch checking of hardened parts.
    • Brinell: castings, annealed and coarse-grain materials.
    • Leeb: portable rebound testing on large parts.
    04

    Process animation

    1. Preparation: polish to Ra ≤ 0.4 µm, remove work-hardened layers.
    2. Mount and align: place the specimen, position the indenter over the test point.
    3. Heat up (hot hardness): evacuate to ≤10⁻² Pa or backfill argon, ramp and soak.
    4. Load: apply force at the set rate, dwell 10–15 s.
    5. Measure: read diagonals or depth, compute HV/HRC.
    6. Gradient: step along depth and plot hardness versus distance.
    0102030405
    05

    Calculation & formulas

    1. Rockwell: HR = K − h/0.002 (K = 100 for HRC, 130 for HRB). At h = 0.078 mm, HRC = 61.

    2. Brinell: HBW = 2F/(πD(D−√(D²−d²))); with F=1838.6 N, D=2.5 mm, d=1.1 mm, HBW ≈ 192.

    3. Vickers: HV = 0.1891·F/d² (F in N); F=9.807 N with d=0.05 mm gives HV ≈ 742.

    4. Test forces: choose Brinell loads by 0.045F/D²; Rockwell 10 kgf preliminary with 60/100/150 kgf total; surface scales 3 / 15/30/45 kgf.

    5. Conversions: HRC ≈ HBW/10 only as a rough mid-range guide — official reports must follow the GB/T 1172 tables.

    06

    Standards

    StandardTitleScope
    GB/T 4340.1-2009Vickers hardness test — test methodVickers
    GB/T 230.1-2018Rockwell hardness testRockwell
    GB/T 231.1-2018Brinell hardness testBrinell
    ISO 6507-1Vickers hardness testExport
    ASTM E92Vickers hardness of metallic materialsAmericas
    GB/T 17394.1-2014Leeb hardness testPortable

    Hot hardness has no unified national standard; ASTM E92 practice is normally cited with temperature, atmosphere, dwell and indenter material stated in the report.

    07

    Selection guide

    1. Principle follows the target: Rockwell for macro hardness and heat-treatment acceptance; Brinell for cast iron, annealed and forged parts where a large indent is representative; Vickers or micro-Vickers for thin layers, coatings and small areas.

    2. Bench or portable: bench units (HRC-150SMJ, HBRVS-187.5) where parts can be brought in; portable Leeb for large moulds, in-service piping and non-removable parts, corrected against a bench reference, typically within ±2 HRC.

    3. One for many: mixed, low-volume shops do well with a Brinell-Vickers-Rockwell combination unit covering HRA/HRB/HRC/HV/HB.

    4. Automation: manual below 100 parts per operator per day; motorised elevation, automatic loading and data upload (HRC-150SMJ) above 200 or for unattended runs.

    5. Reference blocks: two to three blocks covering the working range, checked every shift and sent for annual calibration.

    6. Specimen requirements: Rockwell needs thickness at least ten times the indent depth and Ra ≤1.6 µm; otherwise switch to Vickers or superficial Rockwell.

    ModelPrincipleRangeTypical use
    HRC-150SMJRockwell, motorised digitalHRA/HRB/HRCBatch sampling in heat treatment
    HRC-150SM / HRC-150MRockwellHRA/HRB/HRCIncoming and in-process checks
    HRC-45MSuperficial Rockwell15N/30N/45NSheet, plating, case layers
    HRS-150M / XHRS-150MDigital RockwellHRA/HRB/HRCLines needing data upload
    HBRVS-187.5Brinell-Vickers-RockwellHBW/HRA/HRB/HRC/HVMixed low-volume production

    Three rules for trustworthy data: check the reference block every shift and record it; keep the support face flat and clean; keep indent spacing at least three indent diameters.

    08

    Test method

    Specimen. Test and support faces parallel; thickness at least 1.5 × diagonal (Vickers) or 10 × depth (Rockwell); Ra ≤ 0.4 µm, free of scale and oil.

    Room temperature. Select load, apply within 10–15 s, dwell 10–15 s, unload, measure diagonals. Spacing between indentations ≥3d, from the edge ≥2.5d.

    Hot hardness. Load the specimen, evacuate or backfill argon, ramp and soak 20–30 min, lower the indenter, load and dwell, unload, cool or measure hot, then apply the temperature correction.

    Gradient. Step every 0.05–0.1 mm to the hardness plateau; determine effective case depth at 550 HV1 per GB/T 9450.

    Quality control. Check a certified block (e.g. 700 HV1) each shift, recalibrate beyond ±3%, and log furnace curves and atmosphere for hot tests.

    09

    Industry applications

    • Heat-treatment shops: Rockwell HRC sampling of quenched and tempered parts, carburised surface hardness, Brinell HBW on annealed stock.
    • Castings and forgings: body hardness and HAZ values, section hardness gradients indicating cooling rate and structural uniformity.
    • Moulds and tools: HRC versus wear resistance after hardening and tempering, edge-to-core hardness difference on cutting tools.
    • Thin and small parts: case-hardened layers, coatings and sheet need Vickers or superficial Rockwell (HBRVS-187.5 covers HRA/HRB/HRC/HV/HB).
    • Bearings and gears: ring and raceway hardness, case-to-core difference against carburising requirements.
    • Pressure vessels and piping: weld and HAZ hardness to detect brittle microstructures, typically ≤350 HV10.
    • Incoming verification: hardness as the fastest screening method when material grades are mixed, confirmed by OES.
    • Field and in-service: portable Leeb or ultrasonic hardness testers on large immovable parts, corrected against a bench reference.
    10

    Price and lead time for this model

    By submitting you agree to our privacy policy.

    ⇄0CompareProduct comparison