FAQ

FAQ

Selection guide · Test method

Electronic or hydraulic universal testing machine?

Electronic (servo + ball screw) gives precise speed control up to ~300 kN; hydraulic suits high loads to 2000 kN. Under 100 kN, prefer electronic.

How to choose an extensometer?

Clip-on for high accuracy at low cost; video extensometer for high temperature, thin sheets or fragile specimens; automatic for batch testing. Yield strength requires an extensometer.

Does testing speed affect results?

Yes. Most metals are strain-rate sensitive: faster testing raises yield and tensile strength and lowers elongation. Follow ISO 6892-1 method A or B consistently.

Why do grips and alignment matter?

Eccentric loading adds bending, lowering strength and scattering results. Keep alignment within 10% and verify with an alignment fixture periodically.

How often should the machine be calibrated?

Force annually with a 0.05-class proving instrument at 3–5 points; displacement and speed annually; extensometer every two years. Add interim checks with reference specimens.

⇄0CompareProduct comparison