FAQ

FAQ

Selection guide · Test method

Why must hot hardness be measured in vacuum or inert atmosphere?

Above 600°C the surface oxidises quickly: the oxide layer is far softer than the substrate and thickens with time, so indentation diagonals no longer reflect the base material. Diamond indenters also begin to graphitise above 700°C in air.

The chamber is therefore pumped to ~10⁻² Pa or purged with high-purity argon keeping oxygen below 50 ppm.

Can hot hardness be converted to room-temperature hardness?

No. At temperature the material creeps and the indentation keeps growing with dwell time, so hardness is a function of both temperature and time. Always report temperature, dwell time, atmosphere and indenter type.

How much error does an uneven temperature field cause?

Hardness is strongly temperature dependent — about 2–3 HV per 10°C for aluminium near 300°C. Keep the gradient within ±3°C and ≤5°C across the effective zone around the indentation.

What else can hot indentation measure besides hardness?

One indent also yields elastic modulus from the unloading slope, creep exponent from the dwell segment, indentation fracture toughness, and hardness gradients across coatings or case depth.

Which heating elements reach 1600°C, and how should samples be prepared?

SiC elements reach 1400°C, MoSi₂ reaches 1700°C, graphite works to 2000°C in vacuum or inert gas. Samples: φ20×10 mm or 15×15×8 mm, faces parallel within 0.02 mm, Ra ≤0.2 µm, free of cutting burn.

⇄0CompareProduct comparison