Samples travelled by pneumatic tube to the lab and were analysed on an older spectrometer, six minutes per round trip while the furnace idled, and the long interval made composition correction late.
Solution: TY-9000 installed on the furnace platform with an on-site grinder and argon supply; 40 seconds of grinding and 50 seconds of analysis give C/Si/Mn/P/S/Cr/Ni/Mo in 90 seconds, fed directly to the level-2 system.
Result: six minutes down to 90 seconds, four minutes saved per heat, first-time composition hit rate from 82% to 94%, about 12,000 extra tonnes a year at 1.8 Mt output, with payback in eight months.