Thin-wall tubing2023

One-key flattening and flaring tests on thin-wall stainless tube

WDS10-100 electronic universal machine runs flattening to GB/T 246 and flaring to GB/T 242 on thin-wall tube, displacement resolution 0.001 mm, platen parallelism monitored, report in 5 minutes.

Company
A heat-exchanger equipment plant, E. China
Address
Changzhou, Jiangsu
One-key flattening and flaring tests on thin-wall stainless tube
0.001 mmDisplacement resolution
5 minTime per specimen

The plant flattens and flares 25×1.2 mm thin-wall stainless heat-exchanger tube to GB/T 246 and GB/T 242. The old rig controlled travel by a ruler scale, so flattening height varied and pass/fail calls were often disputed.

Solution: a WDS10-100 computer-controlled electronic universal testing machine, 100 kN class 0.5 with 0.001 mm displacement resolution. The flattening program drives to the standard-specified height and holds for 10 s; flaring uses a 60° conical mandrel at 30 mm/min, with the force-displacement curve recorded throughout.

Result: no cracks at the weld or 90° parent-metal positions after flattening, and a 30% flaring ratio passed; five minutes per specimen with automatic judgement and report output.

Benefit: shipping inspection reports now carry the original curves, and customer acceptance objections fell by about 80%.