Sealing2025

Waviness and Ra control on mechanical seal faces

XZ-230 revealed Ra of 0.08 µm passing while waviness of 0.4 µm failed; after lapping changes the leak rate fell to 0.2%.

Company
Pump manufacturer, Zhejiang
Address
Taizhou, Zhejiang
Waviness and Ra control on mechanical seal faces
0.4 → 0.12 μmWaviness
1.8% → 0.2%Leak rate
0.08 μmRa

Mechanical seal faces need Ra ≤0.1 µm and waviness ≤0.2 µm. Ra always passed, yet high-temperature bench tests occasionally leaked, and teardown showed slight circumferential waviness.

Solution: XZ-230 profilometer with 230 mm travel, four radial and four circumferential traces per face, Gaussian filtering to separate roughness from waviness and evaluate W separately, plus flatness.

Result: Ra of 0.08 µm passed while waviness of 0.4 µm failed, caused by excessive lapping-plate speed producing periodic cutting; lower speed and a spark-out pass brought waviness to 0.12 µm and bench leakage from 1.8% to 0.2%.