Steelmaking2025

90-second furnace analysis shortens steelmaking correction cycles

TY-9000 moves furnace analysis from six minutes in the lab to 90 seconds on the floor, cutting four minutes per heat and adding about 12,000 tonnes a year.

Công ty
Special steel plant, Hebei
Địa chỉ
Tangshan, Hebei
90-second furnace analysis shortens steelmaking correction cycles
6 min → 90 sAnalysis time
-4 minPer heat
82% → 94%Hit rate

Samples travelled by pneumatic tube to the lab and were analysed on an older spectrometer, six minutes per round trip while the furnace idled, and the long interval made composition correction late.

Solution: TY-9000 installed on the furnace platform with an on-site grinder and argon supply; 40 seconds of grinding and 50 seconds of analysis give C/Si/Mn/P/S/Cr/Ni/Mo in 90 seconds, fed directly to the level-2 system.

Result: six minutes down to 90 seconds, four minutes saved per heat, first-time composition hit rate from 82% to 94%, about 12,000 extra tonnes a year at 1.8 Mt output, with payback in eight months.