Chọn vật kính kim tương: đánh đổi NA, độ phân giải và độ sâu trường

Độ phân giải δ=0,61λ/NA tăng theo NA, nhưng độ sâu trường giảm theo 1/NA².

华旋光电技术部
Chọn vật kính kim tương: đánh đổi NA, độ phân giải và độ sâu trường

Core parameter relations

Objective resolution is set by numerical aperture: δ=0.61λ/NA with NA=n·sinα. At green light of 550 nm, a 10×/0.25 resolves about 1.3 μm, a 50×/0.80 about 0.42 μm, and a 100×/0.90 about 0.37 μm. Magnification itself does not add resolution; it only decides whether the eye or camera can see what the objective resolved — the concept of empty magnification: beyond 1000×NA you merely enlarge blur. Depth of field approximates Δz≈n·λ/(2·NA²)+n·e/(M·NA); a 100×/0.90 objective has only about 1 μm, so any specimen tilt defocuses part of the field.

Common grades compared

Mag./NAResolution (μm)Typical use
5×/0.132.5Overview, defect location
10×/0.251.3Routine structure, inclusion survey
20×/0.400.84Structural detail, grain size
50×/0.800.42Fine structure, small precipitates
100×/0.900.37Sub-micron detail, DIC

Aberration correction levels

Achromat objectives correct two colors and keep residual aberrations at the field edge, fine for routine visual work. Plan Achromats add field-flattening for edge-to-edge sharpness, the starting point for photography and image analysis. Plan Fluorite and Plan Apochromat objectives correct three to four colors for faithful color and high contrast at research grade. Metallurgical objectives are infinity-corrected for specimens without cover glass (marked ∞/0); using a biological objective designed for 0.17 mm cover glass badly degrades spherical aberration.

Selection decisions

Working distance fights magnification: 100× objectives often focus closer than 1 mm, so stepped specimens need long-working-distance (LWD) versions. Match magnification to the camera: with 3.45 μm pixels a 50× objective samples at 69 nm, already satisfying Nyquist, and jumping to 100× merely sacrifices field and depth. The rule: adequate is best — prioritize NA and correction class, consider magnification last.