CHWES khai giảng khóa đào tạo chế mẫu kim tương đầu tiên năm 2026

Khóa ba ngày bao gồm cắt, đúc, mài, đánh bóng, tẩm thực và xử lý lỗi.

华旋光电编辑部
CHWES khai giảng khóa đào tạo chế mẫu kim tương đầu tiên năm 2026

Course setup

The first 2026 metallographic preparation course opened at the Shanghai headquarters training center, drawing 26 QC staff from 18 customer organizations. Over three days: day one covers cutting and mounting, including burn prevention and resin selection practice; day two covers polishing sequence design and defect quick-reference; day three is etching, microscopy and grain-size rating practice, with hands-on workstations for every participant.

Course features

All cases come from real industrial scenarios: carburized gear shafts, aluminium die castings and cemented carbide inserts each run a full preparation flow. The troubleshooting segment uses a find-the-defect exercise — instructors prepare specimens containing eight typical defects such as comet tails, relief and edge rounding, and trainees diagnose causes and propose rework under time limits, with the assessment feeding certificate grading.

Outlook

The course runs quarterly, four sessions a year, with free seats for machine purchasers. Session two adds an electropolishing and electro-etching module for stainless and superalloy users. The training material gains a new chapter on image-analysis software, and registration stays open year-round.