Pressure vessels2024

Penetration and intermetallic thickness in stainless-to-carbon steel joints

HX-G3A with measurement software reduces penetration, HAZ width and intermetallic thickness measurement to eight minutes with repeatability within 0.01 mm.

Công ty
Chemical equipment fabricator, Shandong
Địa chỉ
Zibo, Shandong
Danh mục
Kính hiển vi
Penetration and intermetallic thickness in stainless-to-carbon steel joints
8 minPer part
≤1 μmRepeatability
14 μmDeviation caught

Pressure-vessel nozzles join 316L to Q345R. Procedure qualification requires penetration, HAZ width and interfacial Fe-Al intermetallic thickness (≤10 µm). With an upright microscope, tube sections had to be cut and re-mounted, and polishing rounded the interface so the intermetallic layer could not be measured reliably.

Solution: an HX-G3A trinocular inverted stand accepts a 20 mm ring section directly on the stage without mounting; the interface is located at 10× and the intermetallic layer measured at 50×, with software fitting the interface line and averaging thickness.

Result: eight minutes per part, thickness repeatability within 1 µm; two consumable batches showed 14 µm layers traced to excessive heat input and returned to 8 µm after current adjustment. The method is now in the plant welding procedure.

⇄0So sánhSo sánh thông số