Mạ điện2024

Đo vi độ cứng và chiều dày lớp mạ crom cứng

MVSD-1000AE đo crom cứng HV0.1 trên mặt cắt, 950 HV, dày 25 µm.

Công ty
Xưởng mạ crom ty thủy lực, Đông Trung Quốc
Địa chỉ
Diêm Thành, Giang Tô
Đo vi độ cứng và chiều dày lớp mạ crom cứng
950 HV0.1Độ cứng crom
25 μmĐộ dày lớp

Hydraulic rods carry hard chrome requiring hardness of at least 850 HV and thickness of 20-30 µm. Surface indentations suffered substrate influence, and thickness was estimated by eye on a metallurgical microscope, leaving no quantitative basis for supplier grading.

Solution: an MVSD-1000AE fully automatic micro-Vickers hardness tester. Sectioned, mounted and polished specimens are indented at HV0.1 (0.9807 N) with 10 s dwell along the coating depth; indentation-centre-to-interface distances are measured automatically and thickness comes out in the same pass.

Result: the chrome measured 950 HV0.1 at 25 µm thick, with a gradual hardness fall across a 40 µm transition zone; data from five suppliers became directly comparable and one was eliminated.

Benefit: plating acceptance is now quantitative, and early rod-scoring warranty cases fell by 50%.

⇄0So sánhSo sánh thông số