Thân vỏ ô tô2024

CMM cổng Atlas đo kích thước thân xe

CMM Atlas theo ISO 10360-2 đo 320 điểm khe hở trong 45 phút, thay 6 đồ gá chuyên dùng; chuyển mẫu từ 2 tuần còn 1 ngày.

Công ty
Xưởng thân xe, Đông Trung Quốc
Địa chỉ
Thượng Hải
CMM cổng Atlas đo kích thước thân xe
320Điểm mỗi thân xe
45 minChu kỳ đo

Gap and flush on doors, hood and tailgate were checked with 6 dedicated gauges and feeler blades. Each gauge took 12 weeks and over a million yuan to build, gave only pass/fail results, and new-model measurement preparation took two weeks.

Solution: an Atlas gantry CMM with a 5 m x 2.5 m x 1.8 m measuring volume, accepted per ISO 10360-2 with MPE E=±(4+L/250) um. A combined touch-and-scan probe automatically samples 320 functional points on all openings, comparing them with the CAD model and outputting colour deviation maps.

Results: a complete report per body in 45 minutes with 0.05 mm repeatability. All six gauges were retired, saving about 8 million yuan in gauge development and maintenance. Model changeover preparation shrank from two weeks to one day, and the corrective loop for out-of-spec gaps shortened by 60%.

⇄0So sánhSo sánh thông số