The fabricator buys 60 mm plate for vessel skirts requiring Z-direction reduction of area at level Z35 (at least 35%). With no Z-direction tensile capability in-house, every lot went out for testing on a 10-day cycle, seriously disrupting scheduling.

Solution: a WDW200-300 electronic universal testing machine, 300 kN class 0.5, with extended gripping fixtures for Z-direction specimens. Round 10 mm specimens are machined to GB/T 5313, elongation is taken by extensometer, and the software computes reduction of area automatically after fracture.

Result: measured Z-direction reduction of area of 38-44%, meeting Z35; load indication error within ±0.5%, verified to JJG 139.

Benefit: Z-direction results now come out the same day, and thick-plate acceptance fell from 10 days to 1.