Атомное машиностроение2023

Спектрометр TY9000 для поверки труб Inconel 690

Спектрометр TY9000 поверяет химию труб Inconel 690 с точностью 0,01% по Al, Ti; цикл с 3 дней до 4 ч, приемка документов 100%.

Компания
Завод ядерных труб, Вост. Китай
Адрес
Шанхай
Спектрометр TY9000 для поверки труб Inconel 690
0.0005%Предел обнаружения S
4 hЦикл поверки

For Inconel 690 steam-generator tubes, RCC-M requires per-lot recheck of Ni, Cr and Fe plus traces of Al, Ti, C and S. Outsourced wet chemistry took three days, and QA documentation had once been rejected by the inspector over poor traceability.

Solution: a TY9000 full-spectrum OES with a small-sample fixture sparks Φ17 mm tubes directly, achieving 0.05% precision on Ni, Cr, Fe and 0.01% on Al, Ti traces, with a 0.0005% sulfur detection limit. Raw spectra are archived for full traceability per nuclear QA rules.

Results: per-lot recheck completes in 4 hours; deviation against wet chemistry stays within 0.15% Cr and 0.0003% S. QA documentation now passes the inspector first time, saving about 600000 yuan of outsourcing a year and shortening delivery by five days.