Пресс-формы2022

Контроль электродов и вставок пресс-форм

YR3020S: электроды и вставки за 2 мин, повторяемость ≤2 мкм, ремонт EDM с 15% до 3%.

Компания
Завод прецизионных пресс-форм, Юж. Китай
Адрес
Шэньчжэнь, Гуандун
Контроль электродов и вставок пресс-форм
15% → 3%Ремонт EDM
2 minВремя на деталь

Each precision injection mould uses 30-50 graphite electrodes. Wear was checked only on the EDM machine itself and inserts were fitted by micrometer; when an electrode mismatched the cavity, repeated trial burning cost two or three extra days per mould.

Solution: a YR3020S vision machine. Electrodes are datumed on their 3R holders and the profile plus distance to datum faces is measured automatically; inserts are measured on the same machine, and all data are stored against the electrode code so deviations are caught before burning. X/Y indication error is ±(3+L/200) µm.

Result: two minutes per piece with repeatability within 2 µm; pre-inspected electrodes cut EDM rework from 15% to 3%, and first-fit success on inserts improved markedly.

Benefit: mould assembly lead time shortened by 1.5 days on average, and the electrode store now works on a measure-first-use-later rule.

⇄0СравнениеСравнение характеристик