Пресс-формы2024

Равномерность твёрдости H13 после ТО

HBRVS-187.5MV: HRC и HBW на одной машине, 30 с/шт, разброс ≤1,2 HRC.

Компания
Завод литейных форм, Вост. Китай
Адрес
Куньшань, Цзянсу
Категория
Твердомеры
Равномерность твёрдости H13 после ТО
≤1.2 HRCРазброс 9 точек
1 天 → 3 hПартия 20 шт

Die-casting dies in H13 require 44-48 HRC after quenching and tempering, and every block returning from the heat-treat vendor needs a 9-point check. Rockwell and Brinell sat on separate machines, so heavy blocks were handled twice and a 20-block lot took a whole day.

Solution: an HBRVS-187.5MV digital universal hardness tester covering HRC/HBW/HV scales on one machine with up to 187.5 kgf total force. Large blocks are Rockwell-tested directly on the table, and disputed pieces are sectioned for a Brinell re-check, per GB/T 230.1 and GB/T 231.1 respectively.

Result: 30 seconds per piece with the 9-point uniformity spread within 1.2 HRC; a 20-block lot finished in 3 hours, and two blocks reading 2.5 HRC low at corners were rejected before cracking in service.

Benefit: inspection efficiency rose about fivefold, and early die-cracking incidents fell to zero that year.

⇄0СравнениеСравнение характеристик