Auto parts2025

Q6 OES for PMI of Automotive Fastener Wire Rod

Q6 OES identifies 35CrMo, SCM435 and B7 wire rod grades in 5 s at the warehouse with 0.005% carbon precision, replacing spark-eye tests; 4 mix-ups intercepted and OEM line-stops eliminated.

会社名
An automotive fastener maker, E. China
所在地
Jiaxing, Zhejiang
Q6 OES for PMI of Automotive Fastener Wire Rod
0.005%Carbon precision
4 起Mix-ups intercepted

35CrMo and plain 35# wire rods look identical. Reliance on spark-eye checks plus one lab sample per batch once fed 35# into a high-strength bolt line, causing torque failure at the OEM, a line-stop and a 600000-yuan claim.

Solution: a Q6 OES with a wire-rod fixture quantifies C, Si, Mn, Cr, Mo and B in a 5-second spark, with 0.005% carbon precision. The grade library auto-identifies 35CrMo, SCM435, ML20MnTiB and B7 with audible-visual alarms on mismatch.

Results: 100% identification at both receiving and material issue. Four mix-ups were intercepted in the year - two wrong-grade deliveries and two in-store mix-ups. OEM line-stops went to zero, annual quality claims fell from 450000 yuan to nil, and sampling lab cost dropped 70%.

⇄0比較仕様比較