SM-5L Stereo Microscope (上光源)

Stereo Microscope · 上光源

ModelSM-5L
  • 目镜WF10X(Φ20mm)
  • 物镜0.7X~4.5X
  • 放大倍数7X~45X
  • 视场范围Φ28.5~Φ4.5

By submitting you agree to our privacy policy.

01

Overview

SM-5L连续变倍体视显微镜是一种成正像显微镜,采用水平式手轮变倍,具有工作距离长,成像清晰平稳,视场宽阔,操作方便等特点。可广泛应用于文教科研,农林地质,电子精密机械等行业和部门。
一、技术特点:
1、双目观察镜筒45°角倾斜,左右视度可调整。
2、WF10X广角目镜,视场范围可达20mm;
3、物镜从0.7~4.5X连续变倍。选配的附加镜头可以达到0.35X~9X;
4、可以选配环形LED和荧光照明光源;
5、主机结构分为立柱式SM-5LI和挂壁式SM-5LB
二、技术参数:
目镜:WF10X(Φ20mm);
物镜:0.7X~4.5X;
放大倍数:7X~45X;
视场范围:Φ28.5~Φ4.5;
工作距离:88mm;
升降行程:25mm≤H<265mm;
底座尺寸:215X160X60mm;
照明:上光源,12V10W带反光杯亮度可调的卤素灯;
外形尺寸:394*230*160mm;
三、选配组合技术参数SM-5LB:
目镜:WF10X(Φ20mm);
物镜:0.7X~4.5X;
放大倍数:7X~45X;
视场范围:Φ28.5~Φ4.5;
工作距离:88mm;
升降行程:25mm≤H<130mm;
底座尺寸:215X160X60mm;
照明:上光源,12V10W带反光杯亮度可调的卤素灯;
外形尺寸:394*230*160mm;
四、选配件:
目镜:
广角目镜 WF10X(Φ22mm);
广角目镜 WF15X(Φ15mm);
广角目镜 WF20X(Φ12mm);
广角目镜 WF25X(Φ9mm);
分划广角目镜10X(Φ20mm),格值0.1mm/格;
分划广角目镜10X(Φ22mm),格值0.1mm/格;
附加物镜:
0.5X,工作距离:137mm;
0.75X,工作距离:103mm;
1X,工作距离:88mm;
1.5X,工作距离:48mm;
2X,工作距离:29mm;
照明:
8W/90~265V,环形LED照明器工作距离35~200mm;
5W,110V/220V 荧光灯环形照明器;

SM-5L Stereo Microscope (上光源) supplied by CHWES. 9 key specifications available on request.

02

Specifications

目镜WF10X(Φ20mm)
物镜0.7X~4.5X
放大倍数7X~45X
视场范围Φ28.5~Φ4.5
工作距离88mm
升降行程25mm≤H<265mm
底座尺寸215X160X60mm
照明上光源,12V10W带反光杯亮度可调的卤素灯
外形尺寸394*230*160mm

* Generated by rule engine over the product database; for pre-selection only.

03

Working principle

The metallurgical microscope uses an infinity-corrected optical path with reflected Köhler illumination. Light passes the collector, field stop and aperture stop, is deflected by a semi-transparent mirror through the objective onto the specimen, and returns through the same objective to the eyepiece or camera.

  • Bright field for routine microstructure, inclusions and decarburised layers.
  • Dark field collects scattered light to reveal grain boundaries, cracks and non-metallic inclusions.
  • Polarised light identifies anisotropic phases, spheroidised structures and coating stress.
  • DIC converts tiny height differences into contrast, ideal for polished, unetched samples.

Objectives of 5× to 100× are combined with 10× eyepieces. Higher numerical aperture gives better resolution but shallower depth of field.

04

Process animation

  1. Sampling and preparation: sectioning, mounting, grinding, polishing, etching.
  2. Illumination and focus: select BF/DF/POL/DIC and focus.
  3. Image capture: trinocular port, 1× camera adapter, white balance.
  4. Scale calibration: calibrate µm per pixel with a stage micrometer.
  5. Measurement: grain size, case depth, coating thickness, inclusion rating.
0102030405
05

Calculation & formulas

1. System magnification: M = objective × eyepiece × adapter, e.g. 40× / 10× / 1× = 400×.

2. Resolution: d = 0.61λ/NA (λ≈550 nm). A 40× objective with NA 0.65 resolves 0.52 µm; an NA 0.95 dry objective reaches 0.35 µm.

3. Depth of field scales with λ/NA² — higher NA, shallower depth; use low NA for fracture surfaces.

4. Grain size (GB/T 6394): at 100×, grains N per 645 mm² field follow N = 2G−1; counting 128 grains gives G = log2128 + 1 = 8. Intercept method: mean intercept L̄ = line length ÷ intercepts, G = −6.6437 lg L̄ (mm, 100×).

5. Effective case depth: distance to 550 HV1, fitted from a micro-hardness traverse and averaged over three positions.

06

Standards

StandardTitleScope
GB/T 13298-2015Metallic materials — examination of microstructureMicrostructure rating
GB/T 6394-2017Determination of average grain sizeGrain size
ASTM E3-11Guide for metallographic specimen preparationPreparation
ASTM E112Determining average grain sizeGrain size
ISO 643Steels — micrographic determination of grain sizeGrain size

Export projects often require dual GB and ASTM reports; the software ships both rating charts.

07

Selection guide

1. Surface or cross-section: stereo microscopes (HX-ZG7, XSZ) for fracture surfaces, solder joints and coatings; upright or inverted metallurgical microscopes (HX-4, HX-G series) for microstructure, case depth and inclusions.

2. Upright or inverted: upright for small specimens that are flipped often; inverted (HX-G3A/G4C/G5A) for large, heavy parts such as gears, shafts and tube sections that go straight onto the stage without re-mounting.

3. Optics set the ceiling: plan achromats cover routine rating; semi-apochromats or apochromats with a research stand (HX-G5A) are needed for 1000× precipitates and brightfield/darkfield/polarised switching.

4. Three levels of digitalisation: a 5 MP camera for images; camera plus analysis software (grain size, case depth, inclusions, porosity) for automatic rating and reports; motorised stage with scanning and stitching for unattended batches.

5. Do not forget accessories: polariser, darkfield, DIC, and a microhardness interface.

6. Room: an anti-vibration bench at 20±3 °C for research stands; keep preparation and microscopy rooms separate to avoid abrasive dust.

SeriesTypeTypical taskRecommended setup
HX-4A / HX-4BUpright metallurgicalRoutine structure, case depth5×/10×/40× + 5 MP camera
HX-G2A / G2BInvertedBatch samples, no re-mountingBrightfield + simple polariser
HX-G3ATrinocular invertedCase depth, rating, reportsCamera + analysis software
HX-G4C / G5AResearch invertedDarkfield/polarised/DICSemi-apochromat + motorised stage
HX-ZG7 / XSZ-146StereoFracture, solder, low-mag locatingZoom + ring light

Common misconceptions: higher magnification is not better (numerical aperture limits resolution, 100× dry is the practical ceiling); ignoring stage travel so large samples do not fit; buying the stand without software and still rating by eye, which kills repeatability.

08

Test method

Preparation. Section perpendicular to the feature of interest. Keep hot-mounting below 150 °C for aluminium and quenched parts, or use cold mounting. Grind 320→600→800→1200, removing previous scratches at each step; polish with 3 µm then 1 µm diamond. Etchants: 4% nital for carbon steel (3–8 s), aqua regia or electrolytic for stainless, Keller for aluminium.

Examination. Locate a representative field at 5×/10×, then switch to higher power. Rate grain size to GB/T 6394 by comparison or intercept. Measure case depth at 500× with an ocular scale or calibrated software, averaging five readings.

Calibration. Verify µm/pixel daily with a stage micrometer, check against a certified specimen quarterly, record three fields per sample and archive images with scale bars.

Pitfalls. Over-etching widens boundaries and fakes decarburisation; residual scratches can be mistaken for cracks; rounded mounting edges inflate case depth. Keep an unetched specimen for coating and crack review.

09

Industry applications

  • Steel and heat treatment: decarburised depth, carburised/nitrided case depth, grain size (GB/T 6394), non-metallic inclusions (GB/T 10561), banding and Widmanstätten rating.
  • Non-ferrous metals: aluminium grain and recrystallisation, alpha/beta ratio in brass, twinning and corrosion morphology in magnesium.
  • Welding and brazing: penetration, HAZ width, porosity and cracks, intermetallic thickness at dissimilar joints.
  • Additive manufacturing: porosity, lack-of-fusion defects, melt-pool morphology in SLM parts, porosity repeatability within 0.2%.
  • Bearings and gears: martensite rating, retained austenite, carbide network and banding, grinding burn and white layer.
  • Electronics: IMC thickness, plating cross-sections, PCB micro-sections, gold wire ball bonds (stereo plus metallurgical).
  • Powders and ceramics: particle morphology and size, sintered porosity, coating cross-section thickness.
  • Failure analysis: fracture surface macro and micro morphology, corrosion products, crack path and origin, with stereo microscopy for low-magnification locating.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0CompareProduct comparison