PM-11透反射偏光显微镜主要用于鉴别具有双折射特性的物质,是药理学、地质学和机械、冶金等部门用来研究结晶、矿物、岩石和金相组织的重要工具。产品配置无应力平场消色差物镜与大视野目镜,高精度偏光载物台,优良的偏振观察附件等。可在透射偏光、反射偏光与透/反射偏光状态下获得良好的显微图像,仪器机械性能优良,观察舒适,操作方便,是厂矿企业、科研院所进行检测、研究与教学的理想仪器。
一、技术特点:
1、可选透射照明,落射照明或者透反射照明。
2、配置无应力平场物镜(中心可调)与大视野目镜。
3、粗微动同轴调焦机构,粗动松紧可调,带限位锁紧装置,微动格值: 2μm。
4、旋转式载物台,360°等分刻度,游标格值6',中心可调,带锁紧装置,工作台垂直有效行程可达30mm。
5、6V20W卤素灯照明,亮度可调。
6、铰链式观察镜筒,单视度可调,可进行100%透光摄影;
7、推拉式检偏器可360度旋转,带刻度和微动游标;
8、内置推入式勃氏镜,中心可调;
9、λ、λ/4与石英锲补偿器;
10分为PM-11A透射照明、PM-11B透反射照明、PM-11C反射照明三款;
二、技术参数:
光学放大倍数:40~600X、50~600X;
目镜:大视野WF10X(Φ18mm)、分划目镜10X (Φ18mm),0.10mm/格;
PM-11A无应力平场消色差物镜(盖玻片0.17mm)PL:4X/0.10、10X/0.25、40X/0.65(弹簧)、60X/0.85(弹簧);
PM-11B无应力平场消色差物镜(无盖玻片)PLL:5X/0.12、10X/0.25、40X/0.65(弹簧)、60X/0.75(弹簧);
PM-11C无应力平场消色差物镜(无盖玻片)PLL:5X/0.12、10X/0.25、40X/0.65(弹簧)、60X/0.75(弹簧);
目镜筒:三目镜,倾斜30度,可进行100%透光摄影;
PM-11B反射照明:可旋转起偏器、光源6V/20W卤素灯,亮度可调;
PM-11C反射照明:可旋转起偏器、光源6V/20W卤素灯,亮度可调;
PM-11A透射照明:可360度旋转起偏器、有0、90、180、270四个读数,卤素灯照明适用的集光器,光源6V20W卤素灯亮度可调,N.A.1.25可上下升降的阿贝聚光镜;
PM-11B透射照明:可360度旋转起偏器、有0、90、180、270四个读数,卤素灯照明适用的集光器,光源6V20W卤素灯亮度可调,N.A.1.25可上下升降的阿贝聚光镜;
调焦机构:粗微动同轴调焦, 微动格值:2μm,带锁紧和限位装置;
转换器:四孔(内向式滚珠内定位);
载物台:旋转式载物台,直径:Φ150mm,360度等分刻度,游标格值6',中心可调,带锁紧装置;
中间接筒:内置检偏器, 可自由切换正常观察与偏光观察,90°旋转,带刻度,游标格值12';
中间接筒:推入式勃氏镜,中心可调;
中间接筒:λ补偿器;
中间接筒:λ/4补偿器;
中间接筒:石英锲补偿器;
三、选配件:
1、目镜:大视野WF16X(Φ11mm);
2、无应力平场消色差物镜(中心可调、盖玻片0.17mm)PL:20X/0.40、100X/1.25(弹簧、油);
3、无应力平场消色差物镜(中心可调、无盖玻片)PLL:20X/0.40、50X/0.70、80X/0.80、100X/0.85(弹簧、干式);
4、转换器:四孔(外向式滚珠内定位),可调节物镜中心;
5、移动尺:移动范围30*25mm;
6、摄影接口:USB/VIDEO;
7、数码相机接口;
8、CCD适配镜:0.4X/0.5X/1X/0.5X带分划;
PM-11 Polarizing Microscope (透、反射) supplied by CHWES. 11 key specifications available on request.
Specifications
| 光学放大倍数 | 40~600X、50~600X |
|---|---|
| 目镜 | 大视野WF10X(Φ18mm)、分划目镜10X (Φ18mm),0.10mm/格;PM-11A无应力平场消色差物镜(盖玻片0.17mm)PL:4X/0.;10X/0.;40X/0.65(弹簧)、60X/0.85(弹簧) |
| 目镜筒 | 三目镜,倾斜30度,可进行100%透光摄影 |
| PM-11B反射照明 | 可旋转起偏器、光源6V/20W卤素灯,亮度可调 |
| PM-11C反射照明 | 可旋转起偏器、光源6V/20W卤素灯,亮度可调 |
| PM-11A透射照明 | 可360度旋转起偏器、有;1;270四个读数,卤素灯照明适用的集光器,光源6V20W卤素灯亮度可调,N.A.1.25可上下升降的阿贝聚光镜 |
| PM-11B透射照明 | 可360度旋转起偏器、有;1;270四个读数,卤素灯照明适用的集光器,光源6V20W卤素灯亮度可调,N.A.1.25可上下升降的阿贝聚光镜 |
| 调焦机构 | 粗微动同轴调焦, 微动格值:2μm,带锁紧和限位装置 |
| 转换器 | 四孔(内向式滚珠内定位) |
| 载物台 | 旋转式载物台,直径:Φ150mm,360度等分刻度,游标格值6',中心可调,带锁紧装置 |
| 中间接筒 | 内置检偏器, 可自由切换正常观察与偏光观察,90°旋转,带刻度,游标格值12' |
* Generated by rule engine over the product database; for pre-selection only.
Working principle
The metallurgical microscope uses an infinity-corrected optical path with reflected Köhler illumination. Light passes the collector, field stop and aperture stop, is deflected by a semi-transparent mirror through the objective onto the specimen, and returns through the same objective to the eyepiece or camera.
- Bright field for routine microstructure, inclusions and decarburised layers.
- Dark field collects scattered light to reveal grain boundaries, cracks and non-metallic inclusions.
- Polarised light identifies anisotropic phases, spheroidised structures and coating stress.
- DIC converts tiny height differences into contrast, ideal for polished, unetched samples.
Objectives of 5× to 100× are combined with 10× eyepieces. Higher numerical aperture gives better resolution but shallower depth of field.
Process animation
- Sampling and preparation: sectioning, mounting, grinding, polishing, etching.
- Illumination and focus: select BF/DF/POL/DIC and focus.
- Image capture: trinocular port, 1× camera adapter, white balance.
- Scale calibration: calibrate µm per pixel with a stage micrometer.
- Measurement: grain size, case depth, coating thickness, inclusion rating.
Calculation & formulas
1. System magnification: M = objective × eyepiece × adapter, e.g. 40× / 10× / 1× = 400×.
2. Resolution: d = 0.61λ/NA (λ≈550 nm). A 40× objective with NA 0.65 resolves 0.52 µm; an NA 0.95 dry objective reaches 0.35 µm.
3. Depth of field scales with λ/NA² — higher NA, shallower depth; use low NA for fracture surfaces.
4. Grain size (GB/T 6394): at 100×, grains N per 645 mm² field follow N = 2G−1; counting 128 grains gives G = log2128 + 1 = 8. Intercept method: mean intercept L̄ = line length ÷ intercepts, G = −6.6437 lg L̄ (mm, 100×).
5. Effective case depth: distance to 550 HV1, fitted from a micro-hardness traverse and averaged over three positions.
Standards
| Standard | Title | Scope |
|---|---|---|
| GB/T 13298-2015 | Metallic materials — examination of microstructure | Microstructure rating |
| GB/T 6394-2017 | Determination of average grain size | Grain size |
| ASTM E3-11 | Guide for metallographic specimen preparation | Preparation |
| ASTM E112 | Determining average grain size | Grain size |
| ISO 643 | Steels — micrographic determination of grain size | Grain size |
Export projects often require dual GB and ASTM reports; the software ships both rating charts.
Selection guide
1. Surface or cross-section: stereo microscopes (HX-ZG7, XSZ) for fracture surfaces, solder joints and coatings; upright or inverted metallurgical microscopes (HX-4, HX-G series) for microstructure, case depth and inclusions.
2. Upright or inverted: upright for small specimens that are flipped often; inverted (HX-G3A/G4C/G5A) for large, heavy parts such as gears, shafts and tube sections that go straight onto the stage without re-mounting.
3. Optics set the ceiling: plan achromats cover routine rating; semi-apochromats or apochromats with a research stand (HX-G5A) are needed for 1000× precipitates and brightfield/darkfield/polarised switching.
4. Three levels of digitalisation: a 5 MP camera for images; camera plus analysis software (grain size, case depth, inclusions, porosity) for automatic rating and reports; motorised stage with scanning and stitching for unattended batches.
5. Do not forget accessories: polariser, darkfield, DIC, and a microhardness interface.
6. Room: an anti-vibration bench at 20±3 °C for research stands; keep preparation and microscopy rooms separate to avoid abrasive dust.
| Series | Type | Typical task | Recommended setup |
|---|---|---|---|
| HX-4A / HX-4B | Upright metallurgical | Routine structure, case depth | 5×/10×/40× + 5 MP camera |
| HX-G2A / G2B | Inverted | Batch samples, no re-mounting | Brightfield + simple polariser |
| HX-G3A | Trinocular inverted | Case depth, rating, reports | Camera + analysis software |
| HX-G4C / G5A | Research inverted | Darkfield/polarised/DIC | Semi-apochromat + motorised stage |
| HX-ZG7 / XSZ-146 | Stereo | Fracture, solder, low-mag locating | Zoom + ring light |
Common misconceptions: higher magnification is not better (numerical aperture limits resolution, 100× dry is the practical ceiling); ignoring stage travel so large samples do not fit; buying the stand without software and still rating by eye, which kills repeatability.
Test method
Preparation. Section perpendicular to the feature of interest. Keep hot-mounting below 150 °C for aluminium and quenched parts, or use cold mounting. Grind 320→600→800→1200, removing previous scratches at each step; polish with 3 µm then 1 µm diamond. Etchants: 4% nital for carbon steel (3–8 s), aqua regia or electrolytic for stainless, Keller for aluminium.
Examination. Locate a representative field at 5×/10×, then switch to higher power. Rate grain size to GB/T 6394 by comparison or intercept. Measure case depth at 500× with an ocular scale or calibrated software, averaging five readings.
Calibration. Verify µm/pixel daily with a stage micrometer, check against a certified specimen quarterly, record three fields per sample and archive images with scale bars.
Pitfalls. Over-etching widens boundaries and fakes decarburisation; residual scratches can be mistaken for cracks; rounded mounting edges inflate case depth. Keep an unetched specimen for coating and crack review.
Industry applications
- Steel and heat treatment: decarburised depth, carburised/nitrided case depth, grain size (GB/T 6394), non-metallic inclusions (GB/T 10561), banding and Widmanstätten rating.
- Non-ferrous metals: aluminium grain and recrystallisation, alpha/beta ratio in brass, twinning and corrosion morphology in magnesium.
- Welding and brazing: penetration, HAZ width, porosity and cracks, intermetallic thickness at dissimilar joints.
- Additive manufacturing: porosity, lack-of-fusion defects, melt-pool morphology in SLM parts, porosity repeatability within 0.2%.
- Bearings and gears: martensite rating, retained austenite, carbide network and banding, grinding burn and white layer.
- Electronics: IMC thickness, plating cross-sections, PCB micro-sections, gold wire ball bonds (stereo plus metallurgical).
- Powders and ceramics: particle morphology and size, sintered porosity, coating cross-section thickness.
- Failure analysis: fracture surface macro and micro morphology, corrosion products, crack path and origin, with stereo microscopy for low-magnification locating.