Overview

MMAS-16金相显微镜测量分析系统用于对不透明物体的进行显微观察。本仪器配置落射照明器、长距平场消色差物镜(无盖玻片)、大视野目镜和内置偏光观察装置,具有外型美观,操作方便等特点,是金属学、矿物学、精密工程学、电子学等研究的理想器。适用于学校、科研、工厂等部门使用。MMAS-16系统配备了研润自主研发的MMAS测量分析系统以及MOS高端光学系统。
一、技术特点:
1、观察系统:铰链式观察镜筒,30度倾斜,单视度可调。WF10X大视野平场目镜,视场范围直径18mm;10X分化目镜,视场范围18mm,用于校正中心。
2、机械载物台:双层机械式载物台,尺寸210*140mm;移动范围63*50mm。
3、落射照明系统:6V,20W卤素灯,亮度可调。内置视场光阑和孔径光阑、带有黄绿蓝三种滤色片和磨砂玻璃滤色片转换装置,推拉式起偏振器。
4、调焦机构:粗微动同轴调焦机构,粗动松紧可调,带限位锁紧装置,微动格值2um;
5、选配件:
5.1大视野目镜:WF16X(直径11mm);
5.2分划板:10X(直径18mm),格值0.1mm/格;
5.3长距平场消色差物镜(无盖玻璃):PLL40X/0.6、PLL60X/0.75、PLL80X/0.8、PLL100X/0.85(弹簧);
5.4平场消色差物镜(无盖玻璃):PLL100X/1.25(弹簧,油);
5.5适配镜:0.4X、0.5X、1X、0.5带0.1mm/格分化尺;
5.6数码摄像机;
5.7转换器:五孔(内向式滚珠内定位)
二、技术参数:
目镜
大视野 WF10X(Φ18mm)
物镜
长距平场消色差物镜(无盖玻片)PL 5X/0.12
长距平场消色差物镜(无盖玻片)PL L10X/0.25
长距平场消色差物镜(无盖玻片)PL L20X/0.40
长距平场消色差物镜(无盖玻片)PL L50X/0.70
放大倍数
50~500X
目镜筒
三目镜,倾斜30度,(内置检偏振片,可进行切换)
落射照明系统
6V 20W卤素灯,亮度可调
落射照明器带视场光栏、孔径光栏、起偏振片,(黄,蓝,绿)滤色片和磨砂玻璃
调焦机构
粗微动同轴调焦, 微动格值:2μm,粗动松紧可调,带锁紧和限位装置
转换器
四孔(内向式滚珠内定位);
载物台
双层机械移动式(尺寸:210mmX140mm,移动范围:63mmX50mm)
外形尺寸
360*445*200
配备系统
主机+MMAS数据处理系统1套+MOS光学系统一套+电脑一套

MMAS-16 Polarizing Microscope (正置偏光) supplied by CHWES. 9 key specifications available on request.

02

Specifications

物镜长距平场消色差物镜(无盖玻片)PL 5X/0.12
放大倍数50~500X
目镜筒三目镜,倾斜30度,(内置检偏振片,可进行切换)
落射照明系统6V 20W卤素灯,亮度可调
调焦机构粗微动同轴调焦, 微动格值:2μm,粗动松紧可调,带锁紧和限位装置
转换器四孔(内向式滚珠内定位);
载物台双层机械移动式(尺寸:210mmX140mm,移动范围:63mmX50mm)
外形尺寸360*445*200
配备系统主机+MMAS数据处理系统1套+MOS光学系统一套+电脑一套

* Generated by rule engine over the product database; for pre-selection only.

03

Working principle

The metallurgical microscope uses an infinity-corrected optical path with reflected Köhler illumination. Light passes the collector, field stop and aperture stop, is deflected by a semi-transparent mirror through the objective onto the specimen, and returns through the same objective to the eyepiece or camera.

  • Bright field for routine microstructure, inclusions and decarburised layers.
  • Dark field collects scattered light to reveal grain boundaries, cracks and non-metallic inclusions.
  • Polarised light identifies anisotropic phases, spheroidised structures and coating stress.
  • DIC converts tiny height differences into contrast, ideal for polished, unetched samples.

Objectives of 5× to 100× are combined with 10× eyepieces. Higher numerical aperture gives better resolution but shallower depth of field.

04

Process animation

  1. Sampling and preparation: sectioning, mounting, grinding, polishing, etching.
  2. Illumination and focus: select BF/DF/POL/DIC and focus.
  3. Image capture: trinocular port, 1× camera adapter, white balance.
  4. Scale calibration: calibrate µm per pixel with a stage micrometer.
  5. Measurement: grain size, case depth, coating thickness, inclusion rating.
0102030405
05

Calculation & formulas

1. System magnification: M = objective × eyepiece × adapter, e.g. 40× / 10× / 1× = 400×.

2. Resolution: d = 0.61λ/NA (λ≈550 nm). A 40× objective with NA 0.65 resolves 0.52 µm; an NA 0.95 dry objective reaches 0.35 µm.

3. Depth of field scales with λ/NA² — higher NA, shallower depth; use low NA for fracture surfaces.

4. Grain size (GB/T 6394): at 100×, grains N per 645 mm² field follow N = 2G−1; counting 128 grains gives G = log2128 + 1 = 8. Intercept method: mean intercept L̄ = line length ÷ intercepts, G = −6.6437 lg L̄ (mm, 100×).

5. Effective case depth: distance to 550 HV1, fitted from a micro-hardness traverse and averaged over three positions.

06

Standards

StandardTitleScope
GB/T 13298-2015Metallic materials — examination of microstructureMicrostructure rating
GB/T 6394-2017Determination of average grain sizeGrain size
ASTM E3-11Guide for metallographic specimen preparationPreparation
ASTM E112Determining average grain sizeGrain size
ISO 643Steels — micrographic determination of grain sizeGrain size

Export projects often require dual GB and ASTM reports; the software ships both rating charts.

07

Selection guide

1. Surface or cross-section: stereo microscopes (HX-ZG7, XSZ) for fracture surfaces, solder joints and coatings; upright or inverted metallurgical microscopes (HX-4, HX-G series) for microstructure, case depth and inclusions.

2. Upright or inverted: upright for small specimens that are flipped often; inverted (HX-G3A/G4C/G5A) for large, heavy parts such as gears, shafts and tube sections that go straight onto the stage without re-mounting.

3. Optics set the ceiling: plan achromats cover routine rating; semi-apochromats or apochromats with a research stand (HX-G5A) are needed for 1000× precipitates and brightfield/darkfield/polarised switching.

4. Three levels of digitalisation: a 5 MP camera for images; camera plus analysis software (grain size, case depth, inclusions, porosity) for automatic rating and reports; motorised stage with scanning and stitching for unattended batches.

5. Do not forget accessories: polariser, darkfield, DIC, and a microhardness interface.

6. Room: an anti-vibration bench at 20±3 °C for research stands; keep preparation and microscopy rooms separate to avoid abrasive dust.

SeriesTypeTypical taskRecommended setup
HX-4A / HX-4BUpright metallurgicalRoutine structure, case depth5×/10×/40× + 5 MP camera
HX-G2A / G2BInvertedBatch samples, no re-mountingBrightfield + simple polariser
HX-G3ATrinocular invertedCase depth, rating, reportsCamera + analysis software
HX-G4C / G5AResearch invertedDarkfield/polarised/DICSemi-apochromat + motorised stage
HX-ZG7 / XSZ-146StereoFracture, solder, low-mag locatingZoom + ring light

Common misconceptions: higher magnification is not better (numerical aperture limits resolution, 100× dry is the practical ceiling); ignoring stage travel so large samples do not fit; buying the stand without software and still rating by eye, which kills repeatability.

08

Test method

Preparation. Section perpendicular to the feature of interest. Keep hot-mounting below 150 °C for aluminium and quenched parts, or use cold mounting. Grind 320→600→800→1200, removing previous scratches at each step; polish with 3 µm then 1 µm diamond. Etchants: 4% nital for carbon steel (3–8 s), aqua regia or electrolytic for stainless, Keller for aluminium.

Examination. Locate a representative field at 5×/10×, then switch to higher power. Rate grain size to GB/T 6394 by comparison or intercept. Measure case depth at 500× with an ocular scale or calibrated software, averaging five readings.

Calibration. Verify µm/pixel daily with a stage micrometer, check against a certified specimen quarterly, record three fields per sample and archive images with scale bars.

Pitfalls. Over-etching widens boundaries and fakes decarburisation; residual scratches can be mistaken for cracks; rounded mounting edges inflate case depth. Keep an unetched specimen for coating and crack review.

09

Industry applications

  • Steel and heat treatment: decarburised depth, carburised/nitrided case depth, grain size (GB/T 6394), non-metallic inclusions (GB/T 10561), banding and Widmanstätten rating.
  • Non-ferrous metals: aluminium grain and recrystallisation, alpha/beta ratio in brass, twinning and corrosion morphology in magnesium.
  • Welding and brazing: penetration, HAZ width, porosity and cracks, intermetallic thickness at dissimilar joints.
  • Additive manufacturing: porosity, lack-of-fusion defects, melt-pool morphology in SLM parts, porosity repeatability within 0.2%.
  • Bearings and gears: martensite rating, retained austenite, carbide network and banding, grinding burn and white layer.
  • Electronics: IMC thickness, plating cross-sections, PCB micro-sections, gold wire ball bonds (stereo plus metallurgical).
  • Powders and ceramics: particle morphology and size, sintered porosity, coating cross-section thickness.
  • Failure analysis: fracture surface macro and micro morphology, corrosion products, crack path and origin, with stereo microscopy for low-magnification locating.