FM-100 Metallurgical Microscope (倒置、四色)

Metallurgical Microscope · 倒置、四色

ModelFM-100
  • 光学放大倍数100~400X
  • 目镜大视野 WF10X(Φ20mm)
  • 长距平场消色差物镜PLL10X/0.25\工作距离8.;25X/0.4\4.;40X/0.6\3.32(弹簧)
  • 目镜筒三目镜,倾斜30度,可100%通光投影

By submitting you agree to our privacy policy.

01

Overview

FM-100倒置相衬落射荧光显微镜由落射荧光显微系统与倒置生物显微系统组成,配置长工作距离平场物镜与大视野目镜。旋转摆入摆出式聚光系统工作距离长,可对高培养皿或圆筒状烧瓶进行无沾染培养细胞观察,也可以进行相衬观察。落射荧光显微系统采用模块化设计理念,可以安全、快捷地调整照明系统,切换荧光滤色片组件。产品可应用于细胞组织,透明液态组织的显微观察,也可用于生物制药,医学检测、疾病预防等领域内的荧光显微术观察。
一、技术特点:
1、铰链式双目观察镜筒,单视度可调,镜筒30度倾斜;大视野平场目镜,视场范围20mm;
2、可拆卸式移动机械载物台,配备三种不同规格的培养皿托架,适用于不同培养皿观察;
3、摆入摆出式旋转的聚光系统,可对高培养皿或圆筒状烧瓶进行无沾染培养细胞观察;
4、透射照明系统可对光源进行空间调整;
5、落射荧光观察可根据样品检测选择不同的激发光;
6、相衬观察;
二、技术参数:
光学放大倍数:100~400X;
目镜:大视野 WF10X(Φ20mm);
长距平场消色差物镜PLL:10X/0.25\工作距离8.8、25X/0.4\4.78、40X/0.6\3.32(弹簧);
目镜筒:三目镜,倾斜30度,可100%通光投影;
倒置透射照明:6V30W卤素灯,亮度可调;
落射荧光照明:100W高压汞灯;
激发滤色片组:
蓝绿激发滤色片组:蓝激发波长:450~490nm、发射波长:515nm;绿激发波长:495~555nm、发射波长:595nm;
紫外、紫激发滤色片组:紫外激发波长:320~380nm、发射波长:435nm;紫激发波长:380~415nm、发射波长:475nm;
载物台:208*224mm,移动范围79*112mm;
转换器:五孔(滚珠内定位内弯);
相衬装置:
1、特长距平场消色差相衬物镜PLL:10X/0.25\工作距离8.8、25X/0.4\4.78、40X/0.6\3.32(弹簧)PHP2;
2、转轴式相衬装置;
3、对中望远镜;
4、特长工作距离聚光镜:升降可调,NA=0.4,工作距离50mm;
标本架:
1、适合放置Φ68mm或77mmX29mm培养器皿;
2、适合放置128mmX85mm的96孔培养器皿;
3、适合放置82mmX57mm培养器皿;
电源:功率100W, 交流电AC:110V或220V;

FM-100 Metallurgical Microscope (倒置、四色) supplied by CHWES. 16 key specifications available on request.

02

Specifications

光学放大倍数100~400X
目镜大视野 WF10X(Φ20mm)
长距平场消色差物镜PLL10X/0.25\工作距离8.;25X/0.4\4.;40X/0.6\3.32(弹簧)
目镜筒三目镜,倾斜30度,可100%通光投影
倒置透射照明6V30W卤素灯,亮度可调
落射荧光照明100W高压汞灯
蓝绿激发滤色片组蓝激发波长:450~490nm、发射波长:515nm
绿激发波长495~555nm、发射波长:595nm
紫外、紫激发滤色片组紫外激发波长:320~380nm、发射波长:435nm
紫激发波长380~415nm、发射波长:475nm
载物台208*224mm,移动范围79*112mm
转换器五孔(滚珠内定位内弯)
特长距平场消色差相衬物镜PLL10X/0.25\工作距离8.;25X/0.4\4.;40X/0.6\3.32(弹簧)PHP2;转轴式相衬装置;对中望远镜
特长工作距离聚光镜升降可调,NA=0.4,工作距离50mm
标本架适合放置Φ68mm或77mmX29mm培养器皿;适合放置128mmX85mm的96孔培养器皿;适合放置82mmX57mm培养器皿
电源功率100W, 交流电AC:110V或220V

* Generated by rule engine over the product database; for pre-selection only.

03

Working principle

The metallurgical microscope uses an infinity-corrected optical path with reflected Köhler illumination. Light passes the collector, field stop and aperture stop, is deflected by a semi-transparent mirror through the objective onto the specimen, and returns through the same objective to the eyepiece or camera.

  • Bright field for routine microstructure, inclusions and decarburised layers.
  • Dark field collects scattered light to reveal grain boundaries, cracks and non-metallic inclusions.
  • Polarised light identifies anisotropic phases, spheroidised structures and coating stress.
  • DIC converts tiny height differences into contrast, ideal for polished, unetched samples.

Objectives of 5× to 100× are combined with 10× eyepieces. Higher numerical aperture gives better resolution but shallower depth of field.

04

Process animation

  1. Sampling and preparation: sectioning, mounting, grinding, polishing, etching.
  2. Illumination and focus: select BF/DF/POL/DIC and focus.
  3. Image capture: trinocular port, 1× camera adapter, white balance.
  4. Scale calibration: calibrate µm per pixel with a stage micrometer.
  5. Measurement: grain size, case depth, coating thickness, inclusion rating.
0102030405
05

Calculation & formulas

1. System magnification: M = objective × eyepiece × adapter, e.g. 40× / 10× / 1× = 400×.

2. Resolution: d = 0.61λ/NA (λ≈550 nm). A 40× objective with NA 0.65 resolves 0.52 µm; an NA 0.95 dry objective reaches 0.35 µm.

3. Depth of field scales with λ/NA² — higher NA, shallower depth; use low NA for fracture surfaces.

4. Grain size (GB/T 6394): at 100×, grains N per 645 mm² field follow N = 2G−1; counting 128 grains gives G = log2128 + 1 = 8. Intercept method: mean intercept L̄ = line length ÷ intercepts, G = −6.6437 lg L̄ (mm, 100×).

5. Effective case depth: distance to 550 HV1, fitted from a micro-hardness traverse and averaged over three positions.

06

Standards

StandardTitleScope
GB/T 13298-2015Metallic materials — examination of microstructureMicrostructure rating
GB/T 6394-2017Determination of average grain sizeGrain size
ASTM E3-11Guide for metallographic specimen preparationPreparation
ASTM E112Determining average grain sizeGrain size
ISO 643Steels — micrographic determination of grain sizeGrain size

Export projects often require dual GB and ASTM reports; the software ships both rating charts.

07

Selection guide

1. Surface or cross-section: stereo microscopes (HX-ZG7, XSZ) for fracture surfaces, solder joints and coatings; upright or inverted metallurgical microscopes (HX-4, HX-G series) for microstructure, case depth and inclusions.

2. Upright or inverted: upright for small specimens that are flipped often; inverted (HX-G3A/G4C/G5A) for large, heavy parts such as gears, shafts and tube sections that go straight onto the stage without re-mounting.

3. Optics set the ceiling: plan achromats cover routine rating; semi-apochromats or apochromats with a research stand (HX-G5A) are needed for 1000× precipitates and brightfield/darkfield/polarised switching.

4. Three levels of digitalisation: a 5 MP camera for images; camera plus analysis software (grain size, case depth, inclusions, porosity) for automatic rating and reports; motorised stage with scanning and stitching for unattended batches.

5. Do not forget accessories: polariser, darkfield, DIC, and a microhardness interface.

6. Room: an anti-vibration bench at 20±3 °C for research stands; keep preparation and microscopy rooms separate to avoid abrasive dust.

SeriesTypeTypical taskRecommended setup
HX-4A / HX-4BUpright metallurgicalRoutine structure, case depth5×/10×/40× + 5 MP camera
HX-G2A / G2BInvertedBatch samples, no re-mountingBrightfield + simple polariser
HX-G3ATrinocular invertedCase depth, rating, reportsCamera + analysis software
HX-G4C / G5AResearch invertedDarkfield/polarised/DICSemi-apochromat + motorised stage
HX-ZG7 / XSZ-146StereoFracture, solder, low-mag locatingZoom + ring light

Common misconceptions: higher magnification is not better (numerical aperture limits resolution, 100× dry is the practical ceiling); ignoring stage travel so large samples do not fit; buying the stand without software and still rating by eye, which kills repeatability.

08

Test method

Preparation. Section perpendicular to the feature of interest. Keep hot-mounting below 150 °C for aluminium and quenched parts, or use cold mounting. Grind 320→600→800→1200, removing previous scratches at each step; polish with 3 µm then 1 µm diamond. Etchants: 4% nital for carbon steel (3–8 s), aqua regia or electrolytic for stainless, Keller for aluminium.

Examination. Locate a representative field at 5×/10×, then switch to higher power. Rate grain size to GB/T 6394 by comparison or intercept. Measure case depth at 500× with an ocular scale or calibrated software, averaging five readings.

Calibration. Verify µm/pixel daily with a stage micrometer, check against a certified specimen quarterly, record three fields per sample and archive images with scale bars.

Pitfalls. Over-etching widens boundaries and fakes decarburisation; residual scratches can be mistaken for cracks; rounded mounting edges inflate case depth. Keep an unetched specimen for coating and crack review.

09

Industry applications

  • Steel and heat treatment: decarburised depth, carburised/nitrided case depth, grain size (GB/T 6394), non-metallic inclusions (GB/T 10561), banding and Widmanstätten rating.
  • Non-ferrous metals: aluminium grain and recrystallisation, alpha/beta ratio in brass, twinning and corrosion morphology in magnesium.
  • Welding and brazing: penetration, HAZ width, porosity and cracks, intermetallic thickness at dissimilar joints.
  • Additive manufacturing: porosity, lack-of-fusion defects, melt-pool morphology in SLM parts, porosity repeatability within 0.2%.
  • Bearings and gears: martensite rating, retained austenite, carbide network and banding, grinding burn and white layer.
  • Electronics: IMC thickness, plating cross-sections, PCB micro-sections, gold wire ball bonds (stereo plus metallurgical).
  • Powders and ceramics: particle morphology and size, sintered porosity, coating cross-section thickness.
  • Failure analysis: fracture surface macro and micro morphology, corrosion products, crack path and origin, with stereo microscopy for low-magnification locating.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0CompareProduct comparison