Automotive2025

Automated GD&T inspection of e-drive housings

A Spectrum bridge CMM with hybrid probing finished 86 GD&T items in 12 minutes per housing; PPAP passed first time.

Company
EV powertrain plant, East China
Address
Hefei, Anhui
Automated GD&T inspection of e-drive housings
12 minCycle time
1.45Cpk

The e-drive housing packs hole systems with φ0.05–0.10 mm position tolerances, and manual sampling could not keep up with takt time.

Solution: a Spectrum bridge CMM, touch-trigger for holes and scanning for mounting faces, offline-programmed with collision simulation, running unattended at night with reports pushed to MES.

Result: 12 minutes per part (was 40), all 86 GD&T items, Cpk up from 0.9 to 1.45, and first-time PPAP approval.