Precision room-temperature tensile testing of aerospace titanium plate

AGS-X25 250 kN electronic machine measures Rp0.2, Rm and A of TC4 plate to GB/T 228.1 with closed-loop strain-rate control and a class 0.5 extensometer, passing the OEM audit first time.

Company
An aerospace materials processor, SW China
Address
Chengdu, Sichuan
Precision room-temperature tensile testing of aerospace titanium plate
≤5 MPaRp0.2 repeat range
0.00025/sYield-stage rate

The processor must report Rp0.2, Rm, A and Z for every lot of TC4 plate. The old machine ran open-loop speed control, so the yield-stage rate wandered and Rp0.2 repeats differed by up to 15 MPa; the OEM audit demanded correction.

Solution: an AGS-X25 electronic universal testing machine, 250 kN class 0.5, fitted with a 50 mm gauge electronic extensometer calibrated to ISO 9513 class 0.5. GB/T 228.1 method A closed-loop strain-rate control holds the yield-stage rate at 0.00025/s.

Result: TC4 plate measured Rp0.2 of 892 MPa, Rm of 968 MPa and A of 14.5%, with a three-test Rp0.2 range within 5 MPa; the machine passed JJG 139 verification at class 0.5.

Benefit: data passed the OEM audit first time, per-lot in-house testing replaced outsourcing and saved five days per lot.