Fasteners2023

Automated tensile sampling of 12.9 socket-head screws

WAW-300B servo-hydraulic machine with dedicated screw grips auto-judges minimum tensile load per GB/T 3098.1, 3 minutes per piece, 200 pieces per day, class 0.5.

Company
A high-strength fastener plant, E. China
Address
Jiaxing, Zhejiang
Automated tensile sampling of 12.9 socket-head screws
8 → 3 minTime per piece
200 件Daily sampling

The plant makes 12.9-grade socket-head screws from M6 to M16 and samples 8 pieces per lot for tensile testing to GB/T 3098.1. The old machine needed manual gripping and dial reading at eight minutes per piece, with handwritten records that failed the customer data-traceability audit.

Solution: a WAW-300B servo-hydraulic universal testing machine, 300 kN class 0.5 with load indication error within ±0.5%, verified to JJG 139. Dedicated threaded grips with quick centring seats are fitted, and the software carries the GB/T 3098.1 minimum tensile load table, so entering the size triggers automatic pass/fail judgement.

Result: three minutes per piece and 200 pieces per day; maximum load, fracture position and the force-displacement curve are archived automatically into lot reports.

Benefit: zero non-conformities on traceability in the annual customer audit, and sampling manpower halved from two operators to one.

⇄0CompareProduct comparison