Third-party testing2025

Automated preparation doubles per-shift throughput

Q-2 saw, XQ-2B press and MP-2 dual platen raised output from 40 to 85 samples per shift and cut rework from 8% to 2%.

Company
Metal testing laboratory, South China
Address
Guangzhou, Guangdong
Automated preparation doubles per-shift throughput
85Output per shift
2%Rework

The laboratory handles failure analysis for automotive and nuclear clients, with high sample volume and a wide material range from aluminium to nickel superalloys. Manual preparation depended on senior technicians and rework ran at 8%.

Solution: a Q-2 low-speed saw to prevent burning, an XQ-2B dual-station hot press, and an MP-2 dual-platen automatic polisher with programmable force and time, plus four parameter recipes for aluminium, carbon steel, stainless and nickel alloys.

Result: 85 samples per shift, 2% rework, new-staff training cut from three months to three weeks, and 24-hour turnaround for urgent work is now routine.